Effects of reaction melt infiltration temperature on the microstructure and properties of Cf/ZrC-SiC

来源 :特种粉末冶金及复合材料制备/加工第一届学术会议 | 被引量 : 0次 | 上传用户:zty85633278
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  The three-dimensionally carbon fibres reinforced ZrC-SiC matrix composite (Cf/ZrC-SiC) were manufactured by joint processes of precursor infiltration and pyrolysis (PIP) and reactive melt infiltration (RMI).It was found that the SiC phase introduced by PIP process were the main constituent in the carbon bundle.The ZrC phase formed on the edge of pyrolytic carbon by RMI process made residual Zr2Si stayed inside of the matrix.With the increase of the infiltration temperature from 1600 to 1800 ℃, the content of residual Zr2Si alloy in the Cf/ZrC-SiC composites showed an obiously decrease.However, the tensile stress of carbon fibres in the Cf/ZrC-SiC composites increased with the rising infiltration temperature, which would result in more voids in the Cf/ZrC-SiC composite.Besides, the flexural strengths of the composites were comparable with the value obtained by different infiltration temperature.
其他文献
利用DZ-4000(Ⅲ)型电火花沉积/堆焊机,以纳米WC为电极材料,用氩气作为保护气,在NAK80模具钢表面制备了纳米WC沉积层.利用扫描电镜、能谱分析仪、X射线衍射仪和显微硬度计等对沉积层的微结构、元素分布和显微硬度进行了分析.结果表明,利用电火花沉积工艺可获得纳米结构组织涂层,且与基体呈冶金结合.沉积层平均厚度约45μm.沉积层主要由W2C、FeCr相组成,同时含有少量的Co3Fe7相.沉积层
In situ formed AIN particles reinforced magnesium alloy matrix composites was successfully fabricated by bubbling nitrogen gas method.The composites obtained was characterized through X-ray diffractio
利用化学气相沉积法(CVD),分别在光沉积镀铜SiC颗粒和无电镀铜SiC颗粒表面制备石墨烯片和碳纳米管的混合物.利用拉曼光谱和扫描电镜(SEM)研究了制备温度和保温时间对生成的石墨烯片的质量和层数的影响.结果表明:利用化学气相沉积法,均可在无电镀铜SiC颗粒和光沉积镀铜SiC颗粒表面生成多层石墨烯片和碳纳米管的混合物;以无电镀铜颗粒作为基体,在1000℃下保湿20min生成的石墨烯片较佳,已经接近
In the present work, CNTs/Mg composite powders with different deformation degree were prepared, which were used for melting experiment.The deformation mechanism of CNTs/Mg composite powder and the eff
从A356.2铝合金轮毂铸旋坯料中取样,利用电子万能试验机Instron3369进行高温拉伸试验,研究应变速率在0.0001~0.1S-1,变形温度在300~400℃范围内的高温拉伸流变行为.结果表明应变速率与变形温度对该合金流变行为有显著影响,流变应力随温度的降低与应变速率增加而上升.该合金的高温流变行为可用Zener-Hollomon参数描述,通过线性回归计算出变形激活能Q=317.43kJ/
Molecular-dynamics calculations are performed to study the structural changes of a binary Mg-Al alloy cluster containing forty-five Mg atoms and twenty-four Al atoms being at lattice positions of the
本中国硬质合金产业经过60多年发展,从无到有,从小到大,取得了令世界瞩目的成就.从生产规模和产量看,中国已经成为名副其实的硬质合金第一生产大国,但从产业收入及行业利润率来看处在全球同行较低水平,具有典型的"大而不强"的特征.本文通过分析我国硬质合金制造业的现状,以及新背景下我国制造业面临的新形势、新机遇、新挑战,结合《中国制造2025》、国家"十三五"有关规划,指出未来五年硬质合金产业的重点发展趋
To analysis the curing behavior of carbon fiber reinforced epoxy resin prepreg T800/X850, dynamic differential scanning calorimetry (DSC) method was carried out to investigate the cure behaviour of T8
以聚碳硅烷(PCS)和SiC粉为原料,以蛋白质为发泡剂制备泡沫陶瓷坯体,随后在1100℃下进行烧结,制备出了碳化硅泡沫陶瓷.研究了PCS加入量对碳化硅泡沫陶瓷密度、开孔率、弯曲强度和压缩强度的影响.结果表明:随着PCS加入量的增加,制品的密度升高、开孔率降低;而弯曲强度和压缩强度都先增加后降低,当PCS加入量为7.5wt%时达到较大值,二者分别为2.72MPa、4.87MPa,此时开孔率为69.5
本文研究了不同Mo含量Ni3Al粘结金属陶瓷的组织结构和力学性能,研究表明,金属陶瓷表现为芯/环结构硬质相颗粒镶嵌在粘结相中,芯/环结构为黑芯-白环结构.当Mo含量达到15wt%时,出现灰白色外环-亮白色内环-黑芯结构的硬质相颗粒,且随着Mo含量的增加,硬质相颗粒明显细化.液相烧结过程中Mo趋向于在碳化物表面聚集析出,形成富Mo内环相.Ni3Al粘结金属陶瓷的抗弯强度和硬度随Mo含量增加先增大后减