6000-series aluminum alloys with high Cu or excess Si addition were susceptible to intergranular corrosion (IGC).The corrosion behavior of four alloys with different Cu content and Mg/Si was investigated in this study.The four alloys were solution heat treated at 560℃ for 30 min, subsequently quenched in cold water and aged at 180℃ to the peak aging temper.