论文部分内容阅读
GC technology was used to study escaping fluorine in calcined process of mixed rare earth concentrate. The mixed rare earth concentrate and it adding assistant of CaO-NaCl-CaCl2 were calcined at 400~750 ℃ for 30~120 min, and then total amount of fluorine,