The specimens were prepared with high alumina fiber accounting for 0,5%,10% or 15% by mass of the total amount of amorphous silica and high alumina fiber,using
Corundum- spinel purging plugs were optimized through adjusting the formulation and the particle size composition of starting materials to prolong the service l