②图4所示为PDP显示屏驱动集成电路的内部结构,分为逻辑电路和高压驱动电路两部分:逻辑电路负责控制显示屏信号和显示数据;高压驱动电路负责将信号电平移位,并对显示屏施加发光所需的高压脉冲。典型产品有日本NEC公司的UPDl6337和UPDl6305,美国德州仪器公司的SN755831和SN755834。一般而言,寻址驱动集成电路的输出耐压为60~150V,输出电路源—漏电流为30~40mA;扫描电极驱动集成电路的输出耐压为150~200V,输出电路 ② Figure 4 shows the internal structure of the PDP display driver integrated circuit, divided into logic and high-voltage driver circuit of two parts: the logic circuit is responsible for controlling the display signal and display data; high voltage driver circuit is responsible for the signal level shift, and The display applies high voltage pulses required for lighting. Typical products are Japan’s NEC’s UPDl6337 and UPDl6305, the United States Texas Instruments SN755831 and SN755834. In general, the addressing drive IC output withstand voltage of 60 ~ 150V, the output circuit source - the leakage current of 30 ~ 40mA; scan electrode driver integrated circuit output voltage is 150 ~ 200V, the output circuit
其他文献
某型尾翼稳定脱壳式穿甲弹在靶试过程中出现断弹事故,通过系统失效分析,从弹芯与弹芯两结构断裂残体分析及靶场调研,确立弹托为首损件,由断裂特征分析发现加工工艺设计存在缺
高层建筑结构中转换层的形式多种多样,它满足了人们对建筑艺术的需要。在结构施工过程中,转换层是高层建筑结构类型转换的关键节点,具有技术含量高、结构复杂、施工困难的特点。
本文简单介绍了奥地利AICHLIN(艾协林)公司的柔性炉生产线的简单原理及其控制过程,即实现了对渗碳的温度、时间、碳势的全过程控制;从而实现对产品质量的控制与管理.
本文作者通过宏观分析,扫描电镜断口分析及性能检验,结果表明材料正常,断口为一次断裂,其原因与水结应力及温度有关.
采用非平衡磁控溅射及等离子体离子混合注入方法在奥氏体不锈钢1Cr18Ni9Ti基体上制备N/TiN/Ti(N,C)/DLC梯度涂层.研究了类金刚石梯度膜的结构特征和力学性能.试验结果表明,N/
会议
民间借贷作为正规金融之外客观存在的一种经济现象,一直处于各方争议之中。虽然自2007年以来国家先后推行了一系列农村金融新政,引导各类社会资本到农村地区设立村镇银行、贷
本文试验研究了35CrMo钢和T217B钢在室温和-40℃的低温疲劳行为.研究表明,两种钢均循环软化,但在高应变下,35CrMo钢有循环硬化趋势.在低应变长寿命区,环境低温提高了钢的疲劳
会议
目前暖通空调是人们在公共建筑物中常用的一种基础设施。暖通空调施工是建筑施工中的一个重要分部,其安装施工是一个较为复杂的工程,其施工问题直接影响着整个工程的质量和进度
本文采用先低温离子渗氮后再熔盐阳极化的方法在钽表面形成厚度达微米数量级的非晶态层,该层相对于直接阳极化层,组织致密、硬度高、粗糙度低、电阻高.