论文部分内容阅读
Fe-W非晶镀层经铬酸盐钝化处理,可获得具有装饰效果的含Cr钝化膜。经测定,孔蚀电位较钝化前正移1.68V,明显改善了抗CI-腐蚀的能力。AES与XPS的分析结果表明:钝化膜由内外两层构成,外层为Fe(CrO4)3·Cr2(CrO4)3/Cr2(Cr2O7)3·Fe(OH)3/FeOOH·WO3·nH2O等化合物,内层由Cr2O3,CrO3,CrOOH,FeO,Fe2O3及WO3组成。钝化膜厚度约为60nm。该双层饨化膜有效地阻止了Cl-对基体金属的腐蚀。
Chromium passivation of Fe-W amorphous coatings results in a Cr-containing passive film with decorative effect. It was determined that the pitting potential shifted positively to 1.68V before passivation, which markedly improved the resistance to CI-corrosion. The results of AES and XPS show that the passivation film consists of two layers, the outer layer is Fe (CrO4) 3 · Cr2 (CrO4) 3 / Cr2 (Cr2O7) 3 · Fe (OH) 3 / FeOOH · WO3 · nH2O Compound, the inner layer is composed of Cr2O3, CrO3, CrOOH, FeO, Fe2O3 and WO3. Passivation film thickness of about 60nm. The double-layer coating film effectively prevents the corrosion of the base metal by Cl-.