有机添加剂——铜阴极中氢的一个来源

来源 :有色冶炼 | 被引量 : 0次 | 上传用户:singdj
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
铜连铸连轧工艺生产对其原料——电解铜提出了更高的质量要求。而电解铜中氢的存在则被认为是一个影响铜连铸产品质量的最显著的因素。氢与晶粒周围杂质发生协同作用造成在热轧铜材中出现过度的裂纹。本文包括:胶、硫脲这两种主要有机添加剂对阴极超电压的影响和阴极铜中氢含量与电解槽阴极超电压成正比。并提出:实际生产中,最佳超电压范围-30mV以下,在这个范围内,阴极铜杂质氢含量可以维持在1 Copper continuous casting and rolling production of its raw materials - electrolytic copper put forward higher quality requirements. The presence of hydrogen in electrolytic copper is considered to be one of the most significant factors affecting the quality of copper continuous casting products. Hydrogen and grain surrounding the occurrence of synergies resulting in excessive wear in the hot-rolled copper cracks. This article includes: glue, thiourea these two main organic additives on the cathode overvoltage and cathodic copper in the hydrogen content is proportional to the cell cathode overvoltage. And proposed: In actual production, the best over-voltage range -30mV below this range, the cathode copper impurities hydrogen content can be maintained at 1
其他文献
现在苏联国内电热生产中所建造的大型矿热还原电炉的变压器容量达85MVA,自焙电极直径达2000mm。掌握这种大型电炉,技术上还需要解决许多复杂问题,其中主要问题之一是研制运
迄今为止,国外关于回收高炉炉顶放散煤气的报道已有三家。苏联首先于1974年4月在车里雅宾斯克冶金工厂1719m~3的1号高炉上安装了回收炉顶放散煤气的设备,接着日本分别于1979
请下载后查看,本文暂不支持在线获取查看简介。 Please download to view, this article does not support online access to view profile.
患者女性,20岁。发现颈部包块数月,不伴疼痛,无发热。左颈部触及一质地柔软边界欠清的包块,收入院。应用EUB-565A型彩色多普勒显像仪(探头频率7.5MHz)。患者取仰卧位头后仰,于左颈部(包括颈前、后区)查
用液体阳离子交换剂(如羧酸)从浸出液中萃取金属离子时,因至少要加入与被萃金属等当量的碱,一般认为,这种萃取在工业上应用是有妨碍的。除主要的碱费用负担外,将额外的化学
目的:探讨去血供治疗的最佳方法。方法:采用彩色多普勒高频探头检测10只大白兔在肝动脉阻断下门静脉血流的变化。结果:肝动脉阻断后,门静脉血流迅速增加,5~10分钟达到高峰,此后渐恢复,25分钟
本文从合金成分控制、炉渣特性、渣洗去磷、二次造渣、炉外喷粉去磷、硅铬摇包脱磷及全工艺流程磷平衡分析控制含磷量等方面对铬铁脱磷作了初步分析。并扼要介绍了本厂低磷微
患者,男,46岁。因突发左耳闭、耳鸣伴眩晕3天入院。耳鸣为持续性嗡嗡声,视物旋转,走路不稳。就诊后疑为“梅尼埃病”给予烟酰胺加液体静滴、西比灵口服治疗,眩晕症状停止,无自发性眼震
本文主要介绍了太钢50吨氧气顶吹转炉所用的静态控制数学模型(终点控制,供氧,造渣等),它具有较高的命中率和控制精度。该文对建立静态模型中变量的选取,参考炉的选取,模型系
一、概况最近几年来,在氧气转炉炼钢中广泛采用底吹搅拌。林茨钢铁厂和多那耶夫钢铁厂的氧气转炉炼钢车间最近几年也一直采用底吹搅拌。8座转炉全都安装了炉底吹送惰性气体