Users of hot-rolled strip quality requirements more stringent. Thanks to the hydraulic AGC, the strip has sufficient accuracy in the middle except for the head and tail. However, the accuracy of the head is still not ideal. Some head deviations of more than 100um. Although the setting model of the finishing mill has been improved in recent years, the absolute AGC control mode has been developed [1]. However, since the roughing exit