论文部分内容阅读
用振荡声波对黄药溶液和AEA起泡剂乳化液进行预处理后,对纯净矿物(黄铜矿、方铅矿、闪锌矿和黄铁矿)和玢岩铜矿石的矿浆进行了浮选试验。研究表明,溶液在7w/C~2的强度条件下预处理可使黄药氧化,生成3~4%的复黄药,这一现象对浮选过程极为有利。在实验室试验结果的基础上,在法国艾拉济特选矿厂进行了工业试验。结果使铜回收率提高了1.73%,钼回收率提高了1.29%,
After the pretreatment of xanthate solution and AEA foaming agent emulsion with oscillating sound waves, the pulps of pure minerals (chalcopyrite, galena, sphalerite and pyrite) and plutonium copper ore were floated Election test. Studies have shown that the pretreatment of the solution under the condition of 7w / C ~ 2 can oxidize the xanthate to produce 3-4% of the reticulum, which is very beneficial to the flotation process. Based on the results of the laboratory tests, industrial tests were conducted at the Elazig concentrator in France. As a result, the copper recovery rate increased by 1.73%, the molybdenum recovery rate increased by 1.29%