A homemade ball mill was constructed and optimized in order to prepare nano crystallite size of tungsten heavy alloys, with composition of 90W-7Ni-3Fe and 90W-7
Manganese nickel ferrite (Mn0.2Ni0.8Fe2O4) powder was synthesized through oxalate precursor route. The effect of annealing temperature (400℃ - 1100℃) on the f
The thermal stability of nanocrystalline Ni-Co-Fe-P coatings with phosphorus content up to 3.38 wt% prepared by pulsed electrodepostion was studied using XRD, T
Polycrystalline zinc oxide (ZnO) thin films have been deposited at 450°C onto glass and silicon substrates by pulsed laser deposition technique (PLD). The
Three different types of Polyethylene family, High Density Polyethylene, (HDPE), Low Density polyethylene (LDPE) and Linear Low Density polyethylene (LLDPE) pol