【摘 要】
:
Er ions are implanted into the GaN thick films grown by hydride vapor phase epitaxy. The implantation energy is 200 keV and the implantation doses are
【机 构】
:
DepartmentofPhysics,SuzhouUniversityofScienceandTechnology,Suzhou215009,ChinaSuzhouInstituteofNano-T
【出 处】
:
ChineseOpticsLetters
论文部分内容阅读
Er ions are implanted into the GaN thick films grown by hydride vapor phase epitaxy. The implantation energy is 200 keV and the implantation doses are 1×1013, 1×1014, 1×1015, and 5×1015 atom/cm2, respectively. The effects of the implantation dose and annealing temperature on the GaN band-edge luminescence are investigated. The cathodoluminescence spectra from 82 to 323 K are measured for 1×1015 atom/cm2-implanted GaN annealed at 1100°C. Luminescence peaks at 356, 362, 376, 390, and 414 nm are observed on the 82 K cathodoluminescence spectrum. When the temperature is increased to 150 K, the intensities of the 356 and 414 nm peaks are nearly unchanged and the 362, 376, and 390 nm peaks disappear. The intensity ratio of 538 nm (H11/22→I15/24) and 559 nm (S3/24→I15/24) is increased with the increase in temperature. We try to shed light on the above interesting phen
其他文献
Yb3 /Er3 co-doped Na5Lu9F32 single crystals used as a spectral up-converter to improve the power conversion efficiency of perovskite solar cells are prepared via an improved Bridgman approach. Green
提出一种新颖的面向高清电视(HDTV)的微光机电系统(MOEMS)光栅平动式光调制器(GMLM),它利用衍射原理对光进行动态调制,具有较简单的工艺和投影光学系统,其结构适宜形成二维光调制器阵列。针对面向HDTV的应用,提出其指标要求,给出了关键设计公式和设计参数,并设计了符合GMLM特点的加工工艺。最后以加工出来的16×16的GMLM面阵作为激光投影实验对象,验证了GMLM的光学调制原理,证明了加工出的GMLM能够实现对光的动态调制。测量出器件单像素尺寸为52 μm×52 μm,驱动电压6.7 V,对方波
用高温固相法制备了(GdxMyLu0.99-x-y)3Al5O12:1
本文叙述了测试Bow-Tie光纤的拍长和偏振隔离度的简单光学系统和计算方法.
二氧化碳激光器在石汕工业中发现了一种新用途。日本地质学家正用这种激光器向地下烧孔,以代替钻井。
We experimentally investigate the high-order harmonic generation in argon gas cell driven by a multi-cycle broadband infrared laser pulse from a tunable optical-parametric-amplifier (OPA) source. The generation of high-order harmonic continuum with the cu
采用传统的高温固相反应法合成了Tm3 /Yb3 共掺杂Y2(MoO4)3系列荧光粉。XRD结果表明合成的样品为相纯度好的Y2(MoO4)3。在980 nm光激发下, 样品具有较强的位于487 nm和800 nm的蓝色和近红外发射, 同时伴有较弱的位于649 nm的红光发射。它们分别来自于Tm3 的1G4→3H6、3H4→3H6和1G4→3F4跃迁。根据功率相关的上转换发射和能级图分析了Tm3 的上转换发光机制。结果表明, 1G4和3H4能级的布居分别来自于三光子和两光子的能量传递上转换。此外, 随着Tm3
提出了一种改进的基于多尺度变换的红外和可见光图像融合算法。首先, 用形态学帽变换对两幅已经配准的红外图像和可见光图像进行处理, 然后将处理后的图像分别进行轮廓波分解得到一系列的高频图像和低频图像。由于高频图像和低频图像特点的不同, 对高频图像采用平均梯度进行融合, 对低频图像采用PCA的方法进行融合。实验表明, 该方法很好地结合了形态学帽变换、主成分PCA算法和轮廓波变换的优点。与传统的融合方法相比, 提出的融合方法可以提供丰富的图像信息和清晰纹理细节, 且很好地保证了主要目标的亮度基本不变。