Crevice Corrosion Performance of 436 Ferritic Stainless Steel Studied by Different Electrochemical T

来源 :金属学报(英文版) | 被引量 : 0次 | 上传用户:rr_uu
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
The crevice corrosion behaviors of 436 stainless steels in chloride-containing solutions with sulfate addition were studied using potentiodynamic,galvanostatic and repassivation potential measurements.The results of these electrochemical tests were compared and discussed.Galvanostatic test was proved to be the most powerful technique in detecting the crevice corrosion of 436 stainless steels,while the repassivation potential measurement was the most time-saving method in this study.Sulfate ions have inhibited the crevice corrosion of 436 stainless steels in chloride-containing solution,which may result from the effects of competitive adsorption and the IR drop mechanism.
其他文献
In this work,the GaN thin films were directly deposited on multilayer graphene (MLG) by plasma-enhanced atomic layer deposition.The deposition was carried out at a low temperature using triethylgallium (TEGa) precursor and Ar/N2/H2 plasma.Chemical propert
Microstructure and mechanical properties of Ni-28W-6Cr alloy-welded joints produced by gas tungsten arc welding were investigated in this work.Results showed that original fine-grain base metal near fusion line totally transformed into coarse heat affecte
Immiscible alloys have aroused considerable interests in the last decades on account of their special physical and mechanical properties and potential applications.A considerable number of researches have been implemented to investigate the solidification
Hot deformation behavior of a high Al-low Si transformation-induced plasticity (TRIP) steel was studied by an MMS-300 thermo-simulation machine at the temperature range of 1050-1200 ℃ and strain rate range of 0.01-10 s-1.The constitutive equations of the
In a fusion reactor,plasma-facing components (PFCs) will suffer severe thermal shock;behavior and performance of PFCs under high heat flux (HHF) loads are of major importance for the long-term stable operation of the reactor.This work investigates the the
The composition and structural evolution of the corrosion product film of two commercial 90Cu-10Ni tubes,namely Tube A and Tube B,after being immersed in natural seawater for 1,3,and 6 months were characterized by scanning electron microscopy,energy-dispe
The effect of thermal aging on phase transformation and impact toughness of an as-cast duplex stainless steel was investigated at room temperature.After long-term thermal aging,the impact toughness decreases significantly and the cracks initiate and propa
The fracture of pipelines caused by corrosion cracks and the resulting oil and gas leakage can lead to great environmental pollution and economic losses.These negative effects are due to serious corrosion of the plain carbon steels used for armor of flexi
The strain rate sensitivity (SRS) and temperature sensitivity (TS) of 316L austenitic stainless steel were investigated by constant strain rate test (CSRT) and strain rate jump test (SRJT) under four temperatures (293,373,473 and 573 K) and four strain ra
Three-dimensional parts of the 30CrMnSiA steel were successfully fabricated using selective laser melting (SLM).The microstructures and mechanical properties of the SLM-processed 30CrMnSiA samples were investigated by scanning electron microscope and tran