The Pd-modified p-Si electrode was prepared by means of electroless deposition. The average diameter of Pd nanoparticles was about 80 nm from SEM observations.
A 92WC-8Co powder mixture with 33 nm WC grains was prepared by strengthening ball milling and was then sintered by spark plasma sintering (SPS) at 1000- 1200℃