Research on multi-objective optimization of GMAW welding of DH36 steel

来源 :中国焊接 | 被引量 : 0次 | 上传用户:xsnxj112
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
Weld bead morphology plays an important role in welding procedure specification and welding process planning.In order to ob-tain the quantitative relationship between process parameters and weld morphology of DH36 marine steel plate,grey correlation method was used to study multiple morphology characteristics simultaneously.Eighteen experimental runs were proposed according to orthogonal meth-od.With grey correlation theory,three response objectives,aspect ratio,depth of penetration and weld were transformed into a single grey correlation grade (GRG).The process parameters were quantitatively correlated to the GRG value and optimized with the target of maxim-um aspect ratio,minimum depth of penetration and maximum weld area.The results show that the optimized weld bead morphology is bet-ter than other weld bead morphology.The relative error of the predicted GRG with respect to the actual value is 5.06%,which further veri-fies the accuracy of the established model.The microstructure and hardness analysis suggests that the optimized welded joint has obtained required mechanical properties.The research outcomes provide a theoretical basis for multi-objective optimization of arc welding morpho-logy in practical applications.
其他文献
研究钨冶炼废水膜生物反应器(MBR)过程中的微生物菌群特性,旨在为生物法处理钨冶炼废水处理效能的提高提供理论依据.试验结果表明:随盐度的增加污泥体积指数降低,而污泥沉降性能却提高;耐盐驯化期间,化学需氧量(COD)和氨氮(NH4+-N)去除率分别达到了86% ~93%和80% ~85%.微生物需分泌更多的SMP和EPS以抵抗高盐环境下所产生的高渗透压,变形菌门为微生物群落结构的核心菌门,陶厄氏菌属、副球菌属、假单胞菌属、亚硝化单胞菌属和盐单胞菌属为优势菌属.
采用硝酸-氢氟酸-高氯酸将石化工业中常用的难溶钴钼废催化剂快速溶解并利用ICP-OES分析法准确测定样品中有价值的钼和钴元素含量.结果表明:相比于灼烧再酸化,直接采用硝酸-氢氟酸-高氯酸溶解样品更为理想.在仪器最佳测定条件下各元素校准曲线回归方程的线性相关系数均为1,钼和钴的相对标准偏差分别为0.34% 和0.81%,加标回收率均在98% ~101%之间.
采用粉末冶金法制备了系列Mo-Ti-Zr材料.利用拉伸力学性能测试、三点弯曲法测试、OM、SEM等分析测试手段,研究了系列Mo-Ti-Zr材料微观组织与力学性能,结果表明:系列Mo-Ti-Zr材料具有细小的晶粒组织,Zr含量越大,晶粒尺寸越细,硬度越大;Zr含量为1.8%(质量分数,下同)时,材料的室温力学性能最佳,抗拉强度为975 MPa,延伸率为16.7%;Zr含量为0.8%或者1.8%时,试验板材800℃的高温性能最佳,抗拉强度为736 MPa,延伸率为8.3%;Zr含量为1.8%时,材料的抗弯性能
A certain amount of Ti was added to the plasma cladding Fe-Cr-C coating in the early stage in order to improve the quality and properties of the coating.Ti-Fe-Cr-C composite powder was prepared by precursor carbonization-composition process.In situ synthe
煤制天然气残渣(CSNGS)是一种可用于制备地质聚合物的潜在新原料,然而关于用该工业废渣制备地质聚合物的报道却很少.采用机械球磨手段对煤制天然气残渣进行活化改性,分别以氢氧化钠(NaOH)溶液和氢氧化钾(KOH)溶液为激发剂,在不同条件下制备煤制气残渣地质聚合物,并对其强度进行对比.然后,通过X射线粉末衍射仪(XRD)、扫描电镜(SEM)、能谱分析(EDS)以及红外光谱(FT-IR)等微观试验手段对比研究了2种煤制气残渣地质聚合物的微观结构和强度形成机理,并分析了激发剂中不同碱金属阳离子对地质聚合物性能的
The residual deformation in thin-plate butt weldments without wire filling was investigated by simulative and experimental meth-ods.The good consistency on the residual deformation between the simulation result and test measurement data indicates that the
将建筑垃圾再生料用于道路工程建设,是发展绿色低碳交通的具体举措.然而由于再生料成分复杂,在荷载和温度湿度等外界环境的作用下,易发生颗粒破碎,导致再生料的性能不稳定.因此,再生料路基与传统路基也存在明显差异.从建筑垃圾再生料用于路基修筑时的物理力学性能,再生料路基典型工程应用,再生料路基的环保性和经济性等三方面对现有研究成果进行了回顾和梳理.发现目前关于再生料路基的服役性能预估及调控的研究还比较匮乏,少有路基体中污染物对周边环境的影响分析,建议开展此类研究,以便于推进建筑垃圾在路基工程中更为广泛和安全可靠的
钢渣和铁渣是伴随炼钢产生的2种典型固废.目前部分钢渣已被再生用于替代沥青混凝土中的粗骨料.为进一步提高钢渣和铁渣的再利用效率,探讨了采用不同粒径的钢渣和铁渣100%替代沥青混凝土矿料的可行性.首先基于材料微观分析技术以及集料技术指标测试方法,揭示不同粒径钢渣和铁渣的材料特征,确定适合其100%替代沥青混凝土矿料的粒径搭配方案;然后验证方案的可行性,采用Superpave方法设计沥青混凝土,优化拌和工艺,检验沥青混凝土的主要工程性能.结果 表明:钢渣细集料受自身矿物胶凝活性的影响易固结成块,铁渣粗集料的技术
The present paper investigates the welding forming,microstructure and shear tensile test of lap joints with large thickness ratio which were fabricated by laser screw welding (LSW) and resistant spot welding (RSW).The comparison was conducted on two kinds
为研究大掺量钢渣微粉-水泥稳定碎石的性能,采用自制复合激发剂激活钢渣微粉(ASSP),开展了不同胶凝材料剂量(质量分数4%、5%和6%)大掺量(质量分数100%、90%、70%、50%)ASSP水泥稳定碎石的7d无侧限抗压强度(UCS)与5%胶凝材料剂量不同龄期(7,28,90 d)的UCS和劈裂强度(SS)试验;在此基础上,进行了5%胶凝材料剂量100%和70%ASSP-水泥混合料的抗压与劈裂回弹模量、抗冻性、干缩与温缩以及SEM、XRD微观试验,并与对照组P·S· A32.5水泥稳定碎石混合料性能进行