论文部分内容阅读
【摘要】在高层建筑不断增加的过程中,地下室结构施工项目也在不断增加,而混凝土作为建筑工程中较为重要的材料之一,其在地下室结构施工中也属于不可或缺的一项材料,而要想保证地下室结构施工的质量,就一定要确保混凝土性能能够有效地发挥出来,针对这一点,本文主要对地下室混凝土墙体裂缝原因与对策进行了分析,以期能够通过这种方式来提高地下室施工的质量。
【关键词】地下室;混凝土墙体;裂缝原因与对策
Abstract: in the process of high-rise buildings increased, the basement structure construction project is also increasing, and the more important one of the materials as concrete in construction engineering, a material in the basement structure construction also belongs to the indispensable, and to ensure the quality of the basement structure construction, we must ensure that the concrete the performance can effectively play out, on this point, this paper focuses on the basement concrete wall cracks and countermeasures are analyzed, in order to improve the quality of construction of basement in this way.
Key words: basement; concrete wall; crack causes and Countermeasures
0.引言
在近幾年,社会不断发展致使地下施工项目也在不断增加,而地下施工其本身就在一定程度上减少了土地短缺等问题,但是,在地下室施工过程中,其墙体结构大多是采用混凝土,而混凝土施工较为常见的问题就是裂缝这一现象,而一旦出现这问题其就会在很大程度上对地下室结构性能造成影响,同时施工单位还需要对其进行适当的维护,这样都是不符合经济效益。因此,在地下室混凝土墙体施工过程中,一定要尽可能避免混凝土墙体出现裂缝,而针队这一点,笔者主要对裂缝主要特征进行了分析,并且就具体出现裂缝的原因提出了相应的解决对策。
1.地下室混凝土墙体裂缝主要特征分析
地下室混凝土墙体裂缝和普通的墙体裂缝存在着一定的差异性,而其主要的特征包括了以下几点:地下室混凝土墙体出现裂缝现象其大多是出现在附墙柱两端1-2m的位置;地下室混凝土墙体出现裂缝之后,其分布情况大多是平行的,并且还会和地面垂直,但是也还是会有裂缝是倾刹式的,而这种情况下的裂缝其倾刹角度比较小,通常都会小于30°,而其宽度则是小于0.3mm;一般情况下,强度较高的混凝土其出现裂缝的现象也就比较严重,而出现裂缝的时间大多是在拆模不久之后。上述主要的地下室混凝土墙体裂缝主要特征进行了分析,就是希望能够更好地避免这些现象的发生,地下室建筑作为底层工程,其出现裂缝本身就会造成不利影响,如果只是轻微裂缝其只会对建筑外观产生影响,但是,如果裂缝较为严重的话,其就很有可能会对建筑结构安全造成影响,更甚者还会造成建筑陷落、垮塌,最终就会对整个建筑工程结构安全造成影响,同时会有可能会威胁到人体的生命安全。因此,在地下室混凝土结构施工过程中,一定要尽可能避免其墙体出现裂缝。
2.地下室混凝土墙体裂缝原因与对策分析
2.1材料方面所造成的裂缝以及解决对策
地下室混凝土墙体出现裂缝的原因,首先包括了混凝土原材料这一方面,具体主要指的是水泥、砂、石等材料,在实际施工过程中,如果没有做好以下几个方面工作,就很有可能会致使混凝土材料出现质量不合格的现象。比如说,没有对砂的含水率及含泥量进行严格控制;没有对水泥的品种及强度等级进行严格控制;没有对石子品种和粒径进行合理选择;没有对水的各项指标及温度进行严格控制等方面都有可能会让混凝土质量受到影响,从而就会致使地下室混凝土墙体出现裂缝。因此,要想避免地下室混凝土墙体出现裂缝,首先,就需要确保混凝土材料的质量,针对这一点,其需要通过以下几个方面来解决:(1)水泥强度等级一定要高于32.5,并且一定要保证水泥不是过期的,同时也不能使用受潮结块的水泥;(2)在对碎石或卵石的粒径进行选择的过程中,需要控制在5-40mm,在选择砂材料的过程中,最好是选择中砂,并且要确保其含泥量小于3%,而泥块含量要小于1%;(3)在对混凝土进行拌制的过程中,其水一定要确保其属于洁净水;(4)在添加外加剂的过程中,一定要确保其技术性能符合相关标准;(5)在选择粉煤灰的过程中,其等级一定要大于二级,并且掺量要小于20%。
2.2混凝土性能所造成的裂缝以及解决对策
地下室混凝土墙体出现裂缝的原因,除了混凝土材料方面之外,其性能方面也有可能会造成裂缝,而其性能具体就是指混凝土强度等级以及配合比。在施工过程中,混凝土配合比会直接对其性能造成影响,因此,在设计过程中,一定要确保各项材料的隔离性,这样才能确保混凝土具备一定的性能,最终才能减少裂缝出现的次数。针对这一点,在实施施工过程中,其需要做好以下几个方面:(1)水泥使用量一定要大于300kg/m3,并且在添加活性掺合料的过程中,其一定要控制在280kg/m3;(2)在对砂率进行控制的过程中,要将其控制为35-40%;(3)水灰比一定要小于0.55;(4)泵送混凝土坍落度水平构件需要控制在160±10mm,而其竖向构件需要控制在180±10mm,抗渗混凝土则需要控制在100-140mm。 2.3结构设计方面所造成的裂缝以及解决对策
结构设计方面也会成为地下室混凝土墻体出现裂缝的原因之一,地下室混凝土墙体一般情况下都属于超大体积混凝土结构,所以,其有可能会因为附墙柱钢筋较为密集或者是暗柱等自身所存在的收缩应力,进而致使暗柱或附墙柱两侧出现裂缝,因此,在结构设计方面也有可能会造成裂缝。针对这一点,在对其进行解决就需要在设计过程中谨遵以下几点:(1)其外墙混凝土强度等级一定要控制在C25-C35,不能过高也不能过低,并且混凝土厚度还需要大于250mm。(2)在对地下室墙体进行配筋操作的过程中,其一定要满足相应的构造规定,厚度要小于600mm的外墙;水平分布钢筋最小配筋率要控制在0.4-0.5%,而其竖向分布钢筋最小配筋率也需要达到0.3%;在分布过程中其间距一定要小于150mm。(3)在设计过程中,还可以在长墙的暗柱或附墙柱两侧增加水平分布筋,这样就能有效的抵抗混凝土的收缩应力,从而减少两侧出现裂缝的现象。
2.4整体建筑方面所造成的裂缝以及解决对策
整体建筑方面也会成为地下室混凝土墙体出现裂缝的原因之一,在建筑工程项目不断增加的情况下,有些施工单位为了缩短工期降低成本在施工过程中就采用了墙体与顶板整体浇筑混凝土施工方式,从而就致使地下室混凝土墙体出现较多的裂缝,造成这一现象的原因,其主要是因为地上剪力墙其大多是属于短墙肢,这种情况下,混凝土自身收缩应力就很难大于与钢筋共同作用下的抗拉强度,再加上地下室结构又是属于长墙等方面的原因,都会造成温度收缩裂缝的现象。针对这一点,在对其进行控制的过程中,其关键就是要对竖向构件拆模速度以及养护时间进行严格的控制。
2.5混凝土养护方面所造成的裂缝以及解决对策
地下室混凝土墙体出现裂缝,混凝土养护方面也有可能会造成这一现象,混凝土施工完成之后,其只有在一定水分条件之后才能将自身膨胀剂作用发挥出现,因此,对于混凝土的养护就十分的重要,如果没有做好这一项工作,其也会致使混凝土墙体出现裂缝。针对这一点,在对其进行解决的过程中,其一定要确保养护方式以及养护时间的合理性,在对混凝土进行浇筑之后,其一定要在12小时内对其进行覆盖保湿养护,在选择养护剂的过程中,最好是选择一些具备较为良好保水性的产品;如果在养护过程中采用的塑料薄膜养护方式,就一定要确保其覆盖封闭严密性;如果是采用浇水养护则一定要安排专门人员对其进行浇水操作。除此之外,如果施工周期是在冬季,就一定要对其进行适当的防冻措施。
3.结语
综上所述,地下室混凝土墙体出现裂缝的原因较为复杂,而要想避免这一现象的发生,就需要在设计、材料、施工等多方面来进行控制,这样就能有效地减少地下室混凝土墙体出现裂缝。
参考文献:
[1]王桂龙,沈欣.地下室混凝土墙体裂缝成因及对策研究[J].建筑工程技术与设计, 2015,12(17):78-80.
[2]吴金胜.高层建筑地下室混凝土墙体裂缝原因分析及预防措施[J].城市建设理论研究:电子版,2012,36(20):99-100.
作者简介:张伟,1993年4月,男,河南省许昌县人,本科,土木工程专业。
【关键词】地下室;混凝土墙体;裂缝原因与对策
Abstract: in the process of high-rise buildings increased, the basement structure construction project is also increasing, and the more important one of the materials as concrete in construction engineering, a material in the basement structure construction also belongs to the indispensable, and to ensure the quality of the basement structure construction, we must ensure that the concrete the performance can effectively play out, on this point, this paper focuses on the basement concrete wall cracks and countermeasures are analyzed, in order to improve the quality of construction of basement in this way.
Key words: basement; concrete wall; crack causes and Countermeasures
0.引言
在近幾年,社会不断发展致使地下施工项目也在不断增加,而地下施工其本身就在一定程度上减少了土地短缺等问题,但是,在地下室施工过程中,其墙体结构大多是采用混凝土,而混凝土施工较为常见的问题就是裂缝这一现象,而一旦出现这问题其就会在很大程度上对地下室结构性能造成影响,同时施工单位还需要对其进行适当的维护,这样都是不符合经济效益。因此,在地下室混凝土墙体施工过程中,一定要尽可能避免混凝土墙体出现裂缝,而针队这一点,笔者主要对裂缝主要特征进行了分析,并且就具体出现裂缝的原因提出了相应的解决对策。
1.地下室混凝土墙体裂缝主要特征分析
地下室混凝土墙体裂缝和普通的墙体裂缝存在着一定的差异性,而其主要的特征包括了以下几点:地下室混凝土墙体出现裂缝现象其大多是出现在附墙柱两端1-2m的位置;地下室混凝土墙体出现裂缝之后,其分布情况大多是平行的,并且还会和地面垂直,但是也还是会有裂缝是倾刹式的,而这种情况下的裂缝其倾刹角度比较小,通常都会小于30°,而其宽度则是小于0.3mm;一般情况下,强度较高的混凝土其出现裂缝的现象也就比较严重,而出现裂缝的时间大多是在拆模不久之后。上述主要的地下室混凝土墙体裂缝主要特征进行了分析,就是希望能够更好地避免这些现象的发生,地下室建筑作为底层工程,其出现裂缝本身就会造成不利影响,如果只是轻微裂缝其只会对建筑外观产生影响,但是,如果裂缝较为严重的话,其就很有可能会对建筑结构安全造成影响,更甚者还会造成建筑陷落、垮塌,最终就会对整个建筑工程结构安全造成影响,同时会有可能会威胁到人体的生命安全。因此,在地下室混凝土结构施工过程中,一定要尽可能避免其墙体出现裂缝。
2.地下室混凝土墙体裂缝原因与对策分析
2.1材料方面所造成的裂缝以及解决对策
地下室混凝土墙体出现裂缝的原因,首先包括了混凝土原材料这一方面,具体主要指的是水泥、砂、石等材料,在实际施工过程中,如果没有做好以下几个方面工作,就很有可能会致使混凝土材料出现质量不合格的现象。比如说,没有对砂的含水率及含泥量进行严格控制;没有对水泥的品种及强度等级进行严格控制;没有对石子品种和粒径进行合理选择;没有对水的各项指标及温度进行严格控制等方面都有可能会让混凝土质量受到影响,从而就会致使地下室混凝土墙体出现裂缝。因此,要想避免地下室混凝土墙体出现裂缝,首先,就需要确保混凝土材料的质量,针对这一点,其需要通过以下几个方面来解决:(1)水泥强度等级一定要高于32.5,并且一定要保证水泥不是过期的,同时也不能使用受潮结块的水泥;(2)在对碎石或卵石的粒径进行选择的过程中,需要控制在5-40mm,在选择砂材料的过程中,最好是选择中砂,并且要确保其含泥量小于3%,而泥块含量要小于1%;(3)在对混凝土进行拌制的过程中,其水一定要确保其属于洁净水;(4)在添加外加剂的过程中,一定要确保其技术性能符合相关标准;(5)在选择粉煤灰的过程中,其等级一定要大于二级,并且掺量要小于20%。
2.2混凝土性能所造成的裂缝以及解决对策
地下室混凝土墙体出现裂缝的原因,除了混凝土材料方面之外,其性能方面也有可能会造成裂缝,而其性能具体就是指混凝土强度等级以及配合比。在施工过程中,混凝土配合比会直接对其性能造成影响,因此,在设计过程中,一定要确保各项材料的隔离性,这样才能确保混凝土具备一定的性能,最终才能减少裂缝出现的次数。针对这一点,在实施施工过程中,其需要做好以下几个方面:(1)水泥使用量一定要大于300kg/m3,并且在添加活性掺合料的过程中,其一定要控制在280kg/m3;(2)在对砂率进行控制的过程中,要将其控制为35-40%;(3)水灰比一定要小于0.55;(4)泵送混凝土坍落度水平构件需要控制在160±10mm,而其竖向构件需要控制在180±10mm,抗渗混凝土则需要控制在100-140mm。 2.3结构设计方面所造成的裂缝以及解决对策
结构设计方面也会成为地下室混凝土墻体出现裂缝的原因之一,地下室混凝土墙体一般情况下都属于超大体积混凝土结构,所以,其有可能会因为附墙柱钢筋较为密集或者是暗柱等自身所存在的收缩应力,进而致使暗柱或附墙柱两侧出现裂缝,因此,在结构设计方面也有可能会造成裂缝。针对这一点,在对其进行解决就需要在设计过程中谨遵以下几点:(1)其外墙混凝土强度等级一定要控制在C25-C35,不能过高也不能过低,并且混凝土厚度还需要大于250mm。(2)在对地下室墙体进行配筋操作的过程中,其一定要满足相应的构造规定,厚度要小于600mm的外墙;水平分布钢筋最小配筋率要控制在0.4-0.5%,而其竖向分布钢筋最小配筋率也需要达到0.3%;在分布过程中其间距一定要小于150mm。(3)在设计过程中,还可以在长墙的暗柱或附墙柱两侧增加水平分布筋,这样就能有效的抵抗混凝土的收缩应力,从而减少两侧出现裂缝的现象。
2.4整体建筑方面所造成的裂缝以及解决对策
整体建筑方面也会成为地下室混凝土墙体出现裂缝的原因之一,在建筑工程项目不断增加的情况下,有些施工单位为了缩短工期降低成本在施工过程中就采用了墙体与顶板整体浇筑混凝土施工方式,从而就致使地下室混凝土墙体出现较多的裂缝,造成这一现象的原因,其主要是因为地上剪力墙其大多是属于短墙肢,这种情况下,混凝土自身收缩应力就很难大于与钢筋共同作用下的抗拉强度,再加上地下室结构又是属于长墙等方面的原因,都会造成温度收缩裂缝的现象。针对这一点,在对其进行控制的过程中,其关键就是要对竖向构件拆模速度以及养护时间进行严格的控制。
2.5混凝土养护方面所造成的裂缝以及解决对策
地下室混凝土墙体出现裂缝,混凝土养护方面也有可能会造成这一现象,混凝土施工完成之后,其只有在一定水分条件之后才能将自身膨胀剂作用发挥出现,因此,对于混凝土的养护就十分的重要,如果没有做好这一项工作,其也会致使混凝土墙体出现裂缝。针对这一点,在对其进行解决的过程中,其一定要确保养护方式以及养护时间的合理性,在对混凝土进行浇筑之后,其一定要在12小时内对其进行覆盖保湿养护,在选择养护剂的过程中,最好是选择一些具备较为良好保水性的产品;如果在养护过程中采用的塑料薄膜养护方式,就一定要确保其覆盖封闭严密性;如果是采用浇水养护则一定要安排专门人员对其进行浇水操作。除此之外,如果施工周期是在冬季,就一定要对其进行适当的防冻措施。
3.结语
综上所述,地下室混凝土墙体出现裂缝的原因较为复杂,而要想避免这一现象的发生,就需要在设计、材料、施工等多方面来进行控制,这样就能有效地减少地下室混凝土墙体出现裂缝。
参考文献:
[1]王桂龙,沈欣.地下室混凝土墙体裂缝成因及对策研究[J].建筑工程技术与设计, 2015,12(17):78-80.
[2]吴金胜.高层建筑地下室混凝土墙体裂缝原因分析及预防措施[J].城市建设理论研究:电子版,2012,36(20):99-100.
作者简介:张伟,1993年4月,男,河南省许昌县人,本科,土木工程专业。