The deformation behavior of 9 Cr-3 W-3 Co heat-resistant steel at a high-temperature range of 1 060-1 260 ℃ and a strain rate of 0.3 s~(-1) was studied using a Gleeble 3800 heat-simulating test machine. The microstructure and precipitation phases of the s