【摘 要】
:
The spontaneous growth of metal whiskers has been investigated for more than 70 years.However,there is still no agreement on its growth mechanism,and moreover,n
【机 构】
:
Jiangsu Key Laboratory of Advanced Metallic Materials,School of Materials Science and Engineering,So
论文部分内容阅读
The spontaneous growth of metal whiskers has been investigated for more than 70 years.However,there is still no agreement on its growth mechanism,and moreover,new characteristics of this whiskering phenomenon continue to emerge.In this study,Ti2SnC is found to be capable of extracting Sn out of its alloys (SnBi,SnAg) by selectively growing Sn whiskers,and the Sn whiskers share the features of the traditional whiskers on platings and solders.Replacing the Ti2SnC substrate with TiC or SiC,under the same conditions,however,the selective growth of Sn whisker does not happen,which means Ti2SnC plays a critical role in it.Based on the unique crystal structure of Ti2SnC,active Sn atoms diffusing through the basal planes of Ti2SnC is proposed to explain the selectivity.The driving force is suggested to be the high interfacial energy between Ti2SnC and tin.This study is of importance to further understand the growth mechanism of metallic whiskers,and it may be also possible to be harnessed to develop paradigm-shifting technologies of metal purification and metallic whisker/nanowire preparation.
其他文献
Transition metal carbide or nitride (MXene) is regarded as next-generation two-dimensional (2D) mate-rials for various applications,such as photocatalysis,elect
A cost-effective Fe-enriched eutectic high-entropy alloy (EHEA),Fe3sNi2sCr25Mo15,was designed and prepared to avoid the use of expensive Co that is commonly use
The optimization of anode materials such as Sn,P and Sn4P3 in terms of capacity and cyclability is cru-cial to improve the overall performance of sodium-ion bat
Large size polysynthetically twinned crystals of Ti-46Al-8Nb alloy with a parallel lamellar microstructure were successfully prepared using a Ti-43Al-3Si seed b
A low-diffusion NiRePtAl coating ((Ni,Pt)Al outer layer in addition to a Re-rich diffusion barrier layer) was prepared on a Ni3Al-base single crystal (SC) super
The NiCrAlTi coatings free of N and with N incorporations were deposited on austenitic stainless steel 304L by magnetron sputtering in Ar and in gas mixture of
The 93W and Mo1 refractory metals were bonded with different Cu1-xNix coating interlayers of various Ni content using plasma-activated sintering at 700 ℃.The e
The advancement ofsupercapacitors largely relies on the innovation of electrode materials with high-rate performance and ultra-long cycling stability.In this wo
Mg-13.1Gd-1.6Ag-0.4 Zr (wt%) alloy was either iso-thermally extruded at 350 ℃ or differential-thermally extruded with respectively pre-heated billet at 500 ℃ a