Oxide films on Alloy 600 and Alloy 690 formed during exposure to the solution containing 500 ppm B + 2 ppm Li with or without dissolved hydrogen were charac
Operating experience as well as laboratory data have shown that the materials used in reactor internals components for both PWR and BWR are susceptible to i