论文部分内容阅读
日本千叶钢厂6号高炉在原有产量的基础上,为向3号发电站提供足够的高炉煤气,采用高焦比生产炼钢生铁,通过调整风口前吸热量、物料分布、鼓风量,防止铁水中[Si]含量和热损耗上升。操作结果,焦碳能量转换效率达到70~80%。高焦比一般是以提高高炉内热量为目的,或在生产铸造生铁时补充铁水中的[Si]还原热。而6号高炉的高焦比操作则是为了在提高焦碳能量转变效率的基础上,产生更 On the basis of the original output, the No.6 blast furnace at Chiba Plant of Japan provided blast furnace gas to No.3 power station and produced steel-making pig iron with high coke ratio. By adjusting the heat absorption, material distribution and blast volume before the tuyere, Prevent [Si] content and heat loss in hot metal from rising. Operating results, coke energy conversion efficiency of 70 to 80%. High coke ratio is generally based on the purpose of raising the heat in the blast furnace or to replenish the [Si] reduction heat in molten iron when producing pig iron. However, the high coke ratio operation of No.6 blast furnace is based on the increase of coke energy conversion efficiency, resulting in more
其他文献
标准化是一项重要技术基础工作,直接影响工业产品质量和实现产品现代化。粉末冶金制品是一种基础材料和基础零部件。我国粉末冶金工业的技术进步、提高产品质量、发展品种和
前言第二次世界大战期间,为回收核燃料而对萃取过程进行深入研究后,溶剂萃取才发展成一种重要的工业方法(极少例外,特别是石油行业)。从那时起,溶剂萃取在金属的分离、芳香
文献中对铝电解槽工作空间内的质量交换过程的规律性进行了一系列试验研究。已知的计算电流效率的公式中考虑了电流密度、极距、电解槽几何尺寸和电解质温度诸因素。但是,由
纽约Aremco产业有限公司推出一种高强度高熔点的抗高温氧化金属粉末。高纯度的Aremco抗高温粉末的纯度已达到钼99.8%,钽99.9%,钛99.7%,锡99.7%。这些材料的细化程度分别达到
碘络合法是用碘化钾吸收制酸烟气中的汞,然后将含碘汞络合物的吸收液进行电积,使汞析出,碘再生。由于汞电积液成分复杂,各种反应又相互制约,使汞电积受多种因素的影响。韶关
一、前言自1865年平炉炼钢法问世以来,已经历120年了。这期间,平炉炼钢法经过发生、发展的过程,并曾达到兴旺时期,1955年平炉钢占全世界总产钢量的81%。但是,自20世纪50年代
美国的一项专利(专利号№4536212)对用各种原料(氧化铝、铝土矿、粘土)以氯化法炼铝的几个阶段作了改进。美国炼铝的五道工序是:在625—1500℃温度 下进行焙烧,可消除化学结
“瘦肉精”又称盐酸克仑特罗,是一种白色或类白色的结晶粉末,猪食用后在代谢过程中能够促进蛋白质合成,加速脂肪的转化和分解,提高猪肉的瘦肉率。 Clenbuterol, also known
我厂在1985年开始的八万吨锌技术改造配套工程中,积极采用新技术,有计划、有重点地引进国外的先进关键技术和设备。其中,在配料制团工序,从日本引进了一台润式棒磨机。与原
我厂铜电解生产用的始极片系由紫铜模板(俗称种板)以肥皂水作隔离剂在种板槽内电解沉积12—16小时后取出撕下铜皮经铆耳加工制成。以前种板剥离铜皮的作业程序是先用吊车将