递进式脉冲激光沉积CN_x薄膜的组织结构与摩擦学特性

来源 :中国激光 | 被引量 : 0次 | 上传用户:zongbangsheng
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
采用脉冲激光沉积法(PLD)在不同激光通量下烧蚀CNx靶,在单晶硅基底上沉积CNx薄膜。利用扫描电子显微镜(SEM)、X射线能谱仪(EDS)、X射线光电子谱仪(XPS)等对薄膜的形貌、化学成分和微观结构进行了表征。采用球-盘式磨损试验机在大气(相对湿度48%~54%)环境下测试了薄膜的摩擦学特性。结果表明,递进式PLD技术可显著提高CNx薄膜的含氮量。当激光通量从5.0J/cm2提高至10.0J/cm2时,薄膜含氮原子数分数由23.8%上升至29.9%,膜中N-sp2 C键的含量上升,N-sp3 C键和sp3 C-C键的含量下降,薄膜的磨损率从2.1×10-15 m3/(N.m)上升至9.0×10-15 m3/(N.m)。摩擦系数为0.15~0.23,激光通量5.0J/cm2沉积的薄膜有最佳摩擦学性能。 The CNx target was ablated with different laser fluxes by pulsed laser deposition (PLD), and CNx thin films were deposited on monocrystalline silicon substrates. The morphology, chemical composition and microstructure of the films were characterized by scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (EDS) and X-ray photoelectron spectroscopy (XPS) The ball-disc wear tester was used to test the tribological properties of the films in the atmosphere (relative humidity 48% ~ 54%). The results show that the progressive PLD technology can significantly improve the CNx film nitrogen content. When the laser flux increased from 5.0 J / cm2 to 10.0 J / cm2, the content of nitrogen atom in the film increased from 23.8% to 29.9%, and the content of N-sp2 C bond in the film increased. The N-sp3 C bond and sp3 CC Bond content decreased, the wear rate of the film increased from 2.1 × 10-15 m3 / (Nm) to 9.0 × 10-15 m3 / (Nm). The friction coefficient of 0.15 ~ 0.23, laser flux 5.0J / cm2 deposition of the film has the best tribological properties.
其他文献
原发性神经鞘瘤临床上并非少见,但以盆腔肿物为表现形式由妇科收治的患者并不多见.源于后腹膜的神经鞘瘤,有其非特异的临床特征.由于妇科临床医师往往对该病认识的不足,加之缺乏特异性诊断方法,故术前确诊率较低,常使术前准备不足,术中处于被动状态.现将7例原发性腹膜后神经鞘瘤患者的临床资料进行分析如下。
乙基多杀霉素是刺糖菌素类杀虫剂的一个新成员,由美国陶氏益农公司开发。乙基多杀霉素是一高效、广谱性杀虫剂,可用于防治鳞翅目(如小菜蛾、夜蛾、苹果蠹蛾、梨小食心虫、卷