The effects of temperature (0-500℃) on the compressive strength, hardness, average relative density, and microstructure of Ti6Al4V powder green compacts prepar
Intal friction (IF) spectra during reverse martensitic transformation from 35 to 135℃ at different temperature rates of 0.5, 0.75, and 1 ℃/min for Ti50Ni27Cu2