论文部分内容阅读
Nanoparticle hydroxyapatite was prepared by a wet chemical precipitation method. The effects of different synthesis conditions, I.e. Contents of reagents (0.2, 0.5 and 0.8 mol/L), reaction temperatures (20, 37, 55 and 75℃) and reaction time (0-24 h),were