3 mm thick 7050-T7451aluminum alloy joint was obtained by friction stir welding,and the two-step aging treatment was per-formed at 121℃×5 h+163℃×27 h after
The aim of present study is introducing a method by subdividing friction welding phases into three steps according to the temper-ature change during continuous