论文部分内容阅读
In this paper, the newly developed ion exchange phase separation method to create chitosan sub-micron particles is introduced: 1) chitosan was dissolved in a lactic acid aqueous solution. 2) the obtained chitosan solution was added stepwise in a sodium su