论文部分内容阅读
本文利用百度试验法研究了刨花润楠的木材干燥特性,结果表明:刨花润楠属难干木材,干燥速度4级,较慢;截面变形严重,达4级;扭曲明显,为3级;初期开裂和内裂等级分别为1级和2级。参照百度试验缺陷等级以及干燥缺陷对应的干燥条件制定了25~30 mm厚刨花润楠木材干燥基准。
In this paper, Baidu test method was used to study the wood drying properties of Machilus bentis. The results showed that the wood of Machilus thunbergii had a dry speed of 4, which was slow, the cross-section deformity was serious and reached grade 4, the distortion was obvious, Cracking and internal rupture levels were level 1 and level 2, respectively. With reference to Baidu test defect levels and dry conditions corresponding to the drying conditions developed 25-30 mm thick wood shavings Humin timber drying standards.