The shrinkage characteristics of expansive concrete filled steel tube (CFST) are analyzed, Cold shrinkage, creep and autogenous shrinkage are considered as the main reasons of causing CFST contraction. In accordance with the shrinkage characteristics of expansive CFST , a kind of energy-stored delayed expansive agent is exploited, which can not only compensate the shrinkage of the core concrete in every stages, but also make CFST expand according to the delayed expansion mechanism. As the result, the prestress loss will be reduced and expansive energy will be utilized effectively.
The shrinkage characteristics of expansive concrete filled steel tube (CFST) are analyzed, Cold shrinkage, creep and autogenous shrinkage are considered as the main reasons of causing CFST contraction. In accordance with the shrinkage characteristics of expansive CFST, a kind of energy-stored delayed Expansive agent is exploited, which can not only compensate the shrinkage of the core concrete in every stages, but also make CFST expand accordance to the delayed expansion mechanism. As the result, the prestress loss will be reduced and expansive energy will be effectively.