Polyether-polyurethane zwitterionomers based on 4, 4’-diphenylmethane diisocyanate(MDI), methyl diethanolamine (MDEA), and polytetramethylene oxide glycol (PTM
Electrochrometic measurements were carried on the Z-type Langmuir-Blodgett films oftwo liquid crystalline polymers: mono-{6-[4-(phenylazo) naphthyloxy] hexyl} (
The present paper deals with the use of a new polymeric flame retardant material, polyphenylene sulphide (PPS) for plastics. Incorporation of 15—20% PPS into n
Poly(4-methyl-1-pentene) (PMP) hollow fiber membranes were prepared by the melt-spun and cold-stretch(MSCS) method. Scanning electronic microscopy (SEM) was use
A copolymer of bismaleimide-diallylbisphenol A-diphenylsilandiol was synthesized andthe copolymerization was studied by using N-phenylmaleimide, bisphenol A and