转炉冶炼20管用钢经济效益显著

来源 :江西冶金 | 被引量 : 0次 | 上传用户:nestle
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
江西钢厂1983年进行了转炉优钢化工作,转炉冶炼20管用钢7534.94吨,质量达到了电炉钢的水平。钢的含氮量仅为电炉钢的36%,钢中夹杂物总量与电炉钢相当。又由于采用了钢包吹氩的新工艺使钢质更加纯洁、均匀,提高了从荒管到成品的成材率近1%左右。 转炉冶炼20管用钢降低了能源消耗,提高了经济效益。原电炉钢的能耗折合成标准煤为326公斤标准煤/吨钢,转炉为63公斤标 In 1983, Jiangxi Steel Company carried out the excellent converter work of converter, with 7534.94 tons of 20-piece steel used for converter smelting, the quality of which reached the level of electric furnace steel. Nitrogen content of steel is only 36% of EAF, the total amount of inclusions in steel and EAF quite. And because of the new technology of ladle argon blowing, the steel is more pure and uniform, and the finished product yield rate from waste pipe to finished product is increased by nearly 1%. Converter steel smelting 20 to reduce energy consumption and improve economic efficiency. The original electric furnace steel consumption converted into standard coal 326 kg of standard coal / ton of steel, converter 63 kg
其他文献
一、矿床地质条件分层留矿法的新方案曾先后在五个采场中试用。这些采场的地质矿床条件大致相同。矿脉厚度为0.2-0.2米,分支、复合、尖灭及侧现的现象非常普遍,矿石有脆性,
使用卧式转炉吹炼铜冰铜正式投入生产,在我国炼铜史上还是最近几年的事;而关于小型卧式转炉在铜冰铜的吹炼方面的应用,国内外也很少有资料可资查考。我厂经过几年的工业生产
为了了解烧结矿的矿相组成及其结构特征与其强度的关系,进行了碱度(CaO/SiO_2)为0.5~2.0的烧结试验。主要原料是小吴营磁铁精矿、石灰石和煤粉。图1示出烧结矿转鼓强度与碱度
马鞍山钢铁公司1980年以来先后竣工投产了23个节能技术改造项目,形成的节能效果折合标煤6.1×10~4t,在煤气回收、余热利用、工艺及设备的节能改造等各方面取得了成绩,在节能
为了加速鋁工业的发展,适应国民經济的需要,我们除了对鋁生产主要設备电解槽做了一系列的簡化試驗外,还必須对配合鋁生产的輔助生产車間的設备与生产流程同时加以簡化試驗。
出钢带渣会引起回磷,使加入的合金收得率降低、钢包耐火材料熔蚀、钢包精炼效果低。 在出钢时,要求操作者具有相当熟炼的技巧,必须仔细观察转炉中出来的钢流,以便确定准确的
上钢五厂转炉炉衬工段创造了转炉快速砌炉和快速拆炉的经验。使停炉到开炉的时间由原需的50~60小时缩短到22小时,其主要的经验为: (1)快速砌炉: 1)劳动组织的改善: 两个砌炉
本文论述了使用喷射法,用无镁稀土合金作球化剂处理不同含硫量的铁水制备球墨铸铁的可能性。喷射法由于改善了球化反应动力学条件,稀土和镁一样是优良的球化剂。文中对稀土球
吹氩可以净化钢质。顶吹氩优于底吹氩。沸腾钢和一般镇静钢采用吹氮代替吹氩,将显著提高钢的质量。喷吹硅钙粉2公斤/吨,脱硫效率一般达70~90%,[O]在20ppm以下时,[S]可以脱到小
近年来,地方骨干钢铁企业继续贯彻执行国民经济调整方针,加强了能源管理,针对本企业的薄弱环节,采取了一系列有效的节能措施,即使在煤、电供应紧张的不利条件下,能耗仍继续