High temperature corrosion behavior of Si3N4-8%Al2O3(volume fraction) composite ceramics in sulfur-oxygen environments was studied. At 1150℃ and 1350℃,the corrosion processes follow parabolic law with parabolic rate constants (Kp) of 1.45×10-9g2