论文部分内容阅读
对金属板与蜂窝夹层结构复合材料件,成型后在板-板胶接区、蜂窝胶接区产生大量胶瘤的表面成型缺陷进行了改进。通过增加扒皮布、粘贴胶带保护等方法,提高了产品的表面质量,减少了产品表面的补加工,防止对产品强度、后续工序造成影响。
For the metal plate and the honeycomb sandwich composite material, the molding defects on the surface of a large number of the cancellous yarns in the board-plate adhesive area and the honeycomb adhesive area after molding are improved. By increasing the amount of fabric, adhesive tape protection and other methods, to improve the surface quality of the product, reducing the surface of the additional workers, to prevent the product intensity, the impact of subsequent processes.