Ce3+,Eu3+ and Tb3+ singly doped and Ce3+/Eu3+ and Ce3+/Tb3+ co-doped zinc phosphate glasses were prepared by sintering P2O5,ZnO,Ce2(C2O4)3·10H2O and Eu2O3/Tb4O7 mixtures at 1200 °C in the air for 2 h and then annealing at 450 °C for 10 h.Th