论文部分内容阅读
JP2016132753这种用于油、气介质中的仪器零件,由玻璃化转变温度≤25℃的氟橡胶和硫化剂制成。此氟橡胶含有偏二氟乙烯和CH_2:CFRf(Rf=C1~12氟烷基)单体。将氟橡胶100.0份与炭黑20.0份、