讨论了井下特殊环境中最易引起的几种腐蚀形态:电偶腐蚀、应力腐蚀破裂和冲刷腐蚀及其防护途径;分析了矿井空气和矿井水易造成腐蚀的诱因,并提出了防止或减缓腐蚀的对策。
Several kinds of corrosion forms that are most easily caused in special underground environment are discussed: galvanic corrosion, stress corrosion cracking, erosion and protection; the causes of corrosion caused by mine air and mine water are analyzed, and some measures to prevent or mitigate the corrosion Countermeasures.