Ti3 SiC2 materials have been fabricated by spark plasma sintering of the elemental powders with the addi-tion of Al. At the heating rate of 80 ℃/min and under the pressure of 30 MPa, the ideal synthesis temperature ofTi3 SiC2 is in the range of 1 150 - 12