2H-SiC Dendritic Nanocrystals In Situ Formation from Amorphous Silicon Carbide under Electron Beam I

来源 :稀土学报(英文版) | 被引量 : 0次 | 上传用户:qq462283910
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
Under electron beam irradiation, the in-situ formation of 2H-SiC dentritic nanocrystals from amorphous silicon carbide at room temperature was observed. The homogenous transition mainly occurs at the thin edge and on the surface of specimen where the energy obtained from electron beam irradiation is high enough to cause the amorphous crystallizing into 2H-SiC.
其他文献
The creep behavior of directionally solidified (DS) superalloy IC10 was investigated under 192 MPa and 218 MPa at 980 ℃. Under the testing conditions, the mark
The main object of the present research is to make a quantitative evaluation on the microstructure of carbon materials in terms of microcrystal. The digitized i
To investigate the treating parameters influence on the surface roughness of the MAO ceramic coating on AZ91D, experiments were implemented in the alkaline elec
Al2O3/TiAl composites were fabricated by PAXD (pressure-assisted exothermic dispersion) method. The effects of Nb2O5 content on the microstructure and mechanica
Through the addition of rare earth oxides into the coating of electrodes, the high temperature oxidation and sulphidation resistance of weld metal were studied.
Effect of cooling rate on both microstructure and room temperature compressive performance of the AZ91 magnesium alloy was investigated. The experimental result
Honeycomb-like superstructures consisting of ZnS nanosheets with uniform thickness of about 20nm and lateral dimension of several micrometers were built up from
For large-sized AISI P20 steel block used as plastic die with a thickness of more than 200 mm, appropriate quenching processes are the key to obtain much thick
Mg65Cu25Gd10 amorphous alloy powders were synthesized by mechanical alloying (MA). The most suitable process is that the milling velocity is 600 r/min and the m
The evolution of configurations of Aln (n=3,4,6,13,19) clusters were investigated using linear synchronous transit (LST) method. The stable structures of Al3,Al