论文部分内容阅读
摘要:为了有效的对加气砼砌块砌筑以及其抹灰裂缝进行防治和控制,从而确保建筑物的工程质量,文章中介绍了几种加气砼砌块砌筑的墙体在进行抹灰和施工的过程中出现的裂缝,并結合了相关的准则和规范又分别从建筑的设计、所使用的材料以及最后的施工等三个方面提出了如何能够更好的对加气砼砌块砌筑及抹灰裂缝进行有效的控制。
关键词:加气砼砌块;裂缝;控制;防治
Abstract: in order to effectively to aerated concrete block laying and its external thermal insulation crack prevention and control, so as to ensure that the quality of the building project, this paper introduces several aerated concrete block masonry wall plastering and construction in the process of cracks, and combined with the related standards and norms and building design, respectively from the use of materials and the last of the three aspects such as construction can be better put forward how to aerated concrete block laying and crack plastering effective control.
Keywords: aerated concrete block; Crack; Control; Prevention and control
中图分类号: [TQ178] 文献标识码:A 文章编号:
随着城市建设的日益繁荣以及墙体材料改革不断的发展,加气砼砌块以其砌筑方便、密度小、节约能源和土地资源以及导热的系数小等优点已经被广泛的应用在了对围护结构的填充和对非承重的间隔墙上。但是我们缺乏对加气砼的砌块本身相应的了解和研究,这就使得在施工的过程中较容易出现工程的质量问题和施工工艺不够完善的问题,最常见的就是在加气砼砌块进行砌筑时所产生的裂缝,本文就主要针对这些问题展开分析,重点强调一下如何对加气砼砌块在使用的过程中产生的裂缝进行有效控制分析。
一、关于加气砼砌块的特点及产生抹灰裂缝的原因分析
1、加气砼是在高压中的蒸压中形成的,它内部的气孔都是封闭的。如果加气砼的胚体在经过了切割形成块体的过程当中,会破坏了加气砼中气孔的结构,致使它的表面产生一层粉尘,如果不对这些粉尘作出及时的清理,那么在进行抹灰时很容易导致裂缝的产生。
2、加气砼的收缩和变形比较大,尤其是在它出池之后的20多天内,它的收缩和变形达到了最大,在60天之后收缩和变形就基本完成了。如果其收缩变形的时间不够就将其用来砌筑墙体,那么这样也会很容易的导致抹灰时裂缝的产生。
3、加气砼的吸水量比较大但是它吸水后导湿的速度却很慢,如果加气砼砌块进行浇水的时间不够充分,那么它所吸收的水分也就不够充分,那么在砌筑的砂浆和加气砼相遇时,砌筑砂浆中的水分就会被加气砼砌块所吸走,从而较低了砌筑砂浆的强度和硬度,直接的导致结果就是裂缝的产生。
二、加气砼砌块砌筑墙体时存在的质量问题
1、加气砼与抹灰层的粘结不够牢固以及抹灰层的空鼓现象。出现这种现象的主要原因就是:抹灰层没有按照要求施工,一次性的抹灰较厚;砌块的强度和抹灰层的砂浆强度差异较大;加气砼砌块砌筑墙体抹灰前所浇的水没有达到有关的要求;加气砼砌块的表面没有清理干净。
2、砌筑墙面的收缩裂缝的产生。这样裂缝主要是在墙面进行完抹灰之后才产生的。产生的主要原因是:砌筑墙面的抹灰层没有按照有关的要求进行潮湿的养护措施;砌筑的墙面没有设置防裂的措施;抹灰层没有按照有关的规范施工,一次性抹灰过于厚;加气砼砌块的砌筑墙体在进行抹灰前没有按照有关的规定进行浇水。
3、砌筑墙面的温度裂缝的产生。这种裂缝主要是产生在建筑的顶层。这种裂缝会随着温度的变化而发生变化,其产生的主要原因有:对温度变化进行抵抗的措施不够充分;墙面的保温和隔热功能没有达到相关的要求;砌筑的质量不能够达标;砌筑所用的砂浆的强度过低等。
4、加气砼砌块砌筑的墙体与框架的梁和柱直接的交接处产生的裂缝。这种裂缝产生的原因主要有:框架的梁和柱的交接处与砌筑的墙体没有按照有关的要求设置防裂的措施;框架的梁柱与砌筑的墙体之间缝隙太大;拉结筋的设置也不符合相关的要求;加气砼与砼的收缩也不一致。
三、对加气砼砌块砌筑以及抹灰裂缝的有效控制措施
1、在设计和构造中进行控制
我们可以通过各种的构造的措施,提高砌筑墙体的约束能力和整体的性能,从而改善砌筑墙体的防裂和抗裂的能力,达到减少裂缝和防止砌筑墙体产生变形的目的。具体的做法就是:砌筑的墙体其水平的长度不能超过5m或者在墙体的端部没有钢筋混凝土的墙柱的情况下要在墙端或者是墙的中间设置出后浇构造柱,比较长的窗台砌体和阳台维护还应该设置现浇的混凝土构造墙柱,构造柱之间的间距不能超过4m,构造的墙柱应该能够延伸到压顶并且能与混凝土的压顶进行整浇。
2、在对材料的选用上进行控制
(1)加气砼砌块的质量一定要符合相关规程的要求,使用的各种规格的加气砼砌块在其外观的质量、强度和性能方面都应该符合相关的设计和技术要求。加气砼砌块的表面产生裂缝的长度以及缺棱掉角的尺寸都必须在允许的误差范围内,否则在砌块砌筑前要进行相应的修补,比较麻烦。
(2)对加气砼砌块中的含水量进行有效的控制,这样做的目的就是可以很好的减少砌筑的墙体在进行抹灰时产生的裂缝,其具体的做法就是:从每行中的砌筑砌块的竖向的中部各取出一块,并且立即将其装入到塑料的袋中进行密封,然后再进行钻芯的取样。经过取样后,再接着采用接触式的含水量的测试仪器对现场的墙体进行含水量的检测,等到墙体中平均的含水量不大于20%的时候,就可以用砌块进行砌筑了。
(3)较为轻质的砌块的存放时间不能少于28小时,之后才能对墙体进行砌筑,这样做的原因是指如果轻质的砌块存放的时间没有达到规定时间,变形没有相对稳定的话,砌块的收缩性就比较大,立即对其使用容易使墙体很快的收缩并且开裂。
3、关于管理方面的控制措施
(1)在进行施工之前应该认真仔细的做好相应的施工方案和技术的交底,对加气砼砌块砌筑以及抹灰的操作的工艺流程和质量的标准以及控制的相关要点要明确。使得在施工的过程当中各级的施工人员都能够充分的掌握住标准,能够抓住工作的重点。
(2)要严格对样板的领路制度进行执行。在进行大面积的施工之前我们必须要做到先做出样板间和样板墙,然后通过样板再找出可能存在的问题,进而对标准进行明确,从而使得大面积的施工能够有目标和针对性。
(3)对现场质量进行检验的手段要强化,对于工程中所用到的每一种材料都必须经过专人的验收并作及时的检验,只有检验合格之后才能使用,并且我们要根据相应的情况进行随机的抽查,严格的控制不合格的砌筑材料运用在工程当中,每道工序完成之后都要进行中间环节的验收工作,检验合格之后才能够进行下一道工序的执行。
4、要加强监督和检查的力度。各级的质量检测人员都要做到跟踪的调查和检测,重点检查设计以及施工的方案过程中所采取措施的落实情况,而不仅仅只是停留在表面上。
总结:
加气砼砌块砌筑及抹灰裂缝的控制是一项长期的艰巨的任务,我们需要从原材料的使用和生产厂家到设计的单位再到建设与施工整个过程引起高度的重视,各个环节都要密切协调配合,从而为加气砼砌块砌筑能更加广泛的应用提供有利的条件。
参考文献:
[1]王文英.加气砼砌块墙体存在的问题及控制措施[J].中小企业管理与科技,2011(3)
[2]薛复生.加气砼砌块砌筑及抹灰裂缝控制[J].中国房地产业,2011(7)
[3]蒋世清.浅析加气砼砌块的施工技术及管理措施[J].中国科技财富,2010(14)
关键词:加气砼砌块;裂缝;控制;防治
Abstract: in order to effectively to aerated concrete block laying and its external thermal insulation crack prevention and control, so as to ensure that the quality of the building project, this paper introduces several aerated concrete block masonry wall plastering and construction in the process of cracks, and combined with the related standards and norms and building design, respectively from the use of materials and the last of the three aspects such as construction can be better put forward how to aerated concrete block laying and crack plastering effective control.
Keywords: aerated concrete block; Crack; Control; Prevention and control
中图分类号: [TQ178] 文献标识码:A 文章编号:
随着城市建设的日益繁荣以及墙体材料改革不断的发展,加气砼砌块以其砌筑方便、密度小、节约能源和土地资源以及导热的系数小等优点已经被广泛的应用在了对围护结构的填充和对非承重的间隔墙上。但是我们缺乏对加气砼的砌块本身相应的了解和研究,这就使得在施工的过程中较容易出现工程的质量问题和施工工艺不够完善的问题,最常见的就是在加气砼砌块进行砌筑时所产生的裂缝,本文就主要针对这些问题展开分析,重点强调一下如何对加气砼砌块在使用的过程中产生的裂缝进行有效控制分析。
一、关于加气砼砌块的特点及产生抹灰裂缝的原因分析
1、加气砼是在高压中的蒸压中形成的,它内部的气孔都是封闭的。如果加气砼的胚体在经过了切割形成块体的过程当中,会破坏了加气砼中气孔的结构,致使它的表面产生一层粉尘,如果不对这些粉尘作出及时的清理,那么在进行抹灰时很容易导致裂缝的产生。
2、加气砼的收缩和变形比较大,尤其是在它出池之后的20多天内,它的收缩和变形达到了最大,在60天之后收缩和变形就基本完成了。如果其收缩变形的时间不够就将其用来砌筑墙体,那么这样也会很容易的导致抹灰时裂缝的产生。
3、加气砼的吸水量比较大但是它吸水后导湿的速度却很慢,如果加气砼砌块进行浇水的时间不够充分,那么它所吸收的水分也就不够充分,那么在砌筑的砂浆和加气砼相遇时,砌筑砂浆中的水分就会被加气砼砌块所吸走,从而较低了砌筑砂浆的强度和硬度,直接的导致结果就是裂缝的产生。
二、加气砼砌块砌筑墙体时存在的质量问题
1、加气砼与抹灰层的粘结不够牢固以及抹灰层的空鼓现象。出现这种现象的主要原因就是:抹灰层没有按照要求施工,一次性的抹灰较厚;砌块的强度和抹灰层的砂浆强度差异较大;加气砼砌块砌筑墙体抹灰前所浇的水没有达到有关的要求;加气砼砌块的表面没有清理干净。
2、砌筑墙面的收缩裂缝的产生。这样裂缝主要是在墙面进行完抹灰之后才产生的。产生的主要原因是:砌筑墙面的抹灰层没有按照有关的要求进行潮湿的养护措施;砌筑的墙面没有设置防裂的措施;抹灰层没有按照有关的规范施工,一次性抹灰过于厚;加气砼砌块的砌筑墙体在进行抹灰前没有按照有关的规定进行浇水。
3、砌筑墙面的温度裂缝的产生。这种裂缝主要是产生在建筑的顶层。这种裂缝会随着温度的变化而发生变化,其产生的主要原因有:对温度变化进行抵抗的措施不够充分;墙面的保温和隔热功能没有达到相关的要求;砌筑的质量不能够达标;砌筑所用的砂浆的强度过低等。
4、加气砼砌块砌筑的墙体与框架的梁和柱直接的交接处产生的裂缝。这种裂缝产生的原因主要有:框架的梁和柱的交接处与砌筑的墙体没有按照有关的要求设置防裂的措施;框架的梁柱与砌筑的墙体之间缝隙太大;拉结筋的设置也不符合相关的要求;加气砼与砼的收缩也不一致。
三、对加气砼砌块砌筑以及抹灰裂缝的有效控制措施
1、在设计和构造中进行控制
我们可以通过各种的构造的措施,提高砌筑墙体的约束能力和整体的性能,从而改善砌筑墙体的防裂和抗裂的能力,达到减少裂缝和防止砌筑墙体产生变形的目的。具体的做法就是:砌筑的墙体其水平的长度不能超过5m或者在墙体的端部没有钢筋混凝土的墙柱的情况下要在墙端或者是墙的中间设置出后浇构造柱,比较长的窗台砌体和阳台维护还应该设置现浇的混凝土构造墙柱,构造柱之间的间距不能超过4m,构造的墙柱应该能够延伸到压顶并且能与混凝土的压顶进行整浇。
2、在对材料的选用上进行控制
(1)加气砼砌块的质量一定要符合相关规程的要求,使用的各种规格的加气砼砌块在其外观的质量、强度和性能方面都应该符合相关的设计和技术要求。加气砼砌块的表面产生裂缝的长度以及缺棱掉角的尺寸都必须在允许的误差范围内,否则在砌块砌筑前要进行相应的修补,比较麻烦。
(2)对加气砼砌块中的含水量进行有效的控制,这样做的目的就是可以很好的减少砌筑的墙体在进行抹灰时产生的裂缝,其具体的做法就是:从每行中的砌筑砌块的竖向的中部各取出一块,并且立即将其装入到塑料的袋中进行密封,然后再进行钻芯的取样。经过取样后,再接着采用接触式的含水量的测试仪器对现场的墙体进行含水量的检测,等到墙体中平均的含水量不大于20%的时候,就可以用砌块进行砌筑了。
(3)较为轻质的砌块的存放时间不能少于28小时,之后才能对墙体进行砌筑,这样做的原因是指如果轻质的砌块存放的时间没有达到规定时间,变形没有相对稳定的话,砌块的收缩性就比较大,立即对其使用容易使墙体很快的收缩并且开裂。
3、关于管理方面的控制措施
(1)在进行施工之前应该认真仔细的做好相应的施工方案和技术的交底,对加气砼砌块砌筑以及抹灰的操作的工艺流程和质量的标准以及控制的相关要点要明确。使得在施工的过程当中各级的施工人员都能够充分的掌握住标准,能够抓住工作的重点。
(2)要严格对样板的领路制度进行执行。在进行大面积的施工之前我们必须要做到先做出样板间和样板墙,然后通过样板再找出可能存在的问题,进而对标准进行明确,从而使得大面积的施工能够有目标和针对性。
(3)对现场质量进行检验的手段要强化,对于工程中所用到的每一种材料都必须经过专人的验收并作及时的检验,只有检验合格之后才能使用,并且我们要根据相应的情况进行随机的抽查,严格的控制不合格的砌筑材料运用在工程当中,每道工序完成之后都要进行中间环节的验收工作,检验合格之后才能够进行下一道工序的执行。
4、要加强监督和检查的力度。各级的质量检测人员都要做到跟踪的调查和检测,重点检查设计以及施工的方案过程中所采取措施的落实情况,而不仅仅只是停留在表面上。
总结:
加气砼砌块砌筑及抹灰裂缝的控制是一项长期的艰巨的任务,我们需要从原材料的使用和生产厂家到设计的单位再到建设与施工整个过程引起高度的重视,各个环节都要密切协调配合,从而为加气砼砌块砌筑能更加广泛的应用提供有利的条件。
参考文献:
[1]王文英.加气砼砌块墙体存在的问题及控制措施[J].中小企业管理与科技,2011(3)
[2]薛复生.加气砼砌块砌筑及抹灰裂缝控制[J].中国房地产业,2011(7)
[3]蒋世清.浅析加气砼砌块的施工技术及管理措施[J].中国科技财富,2010(14)