论文部分内容阅读
<正>The RE-aluminized coating and pure aluminized coating on 20 carbons steel were prepared by hot dip aluminizing method at 740℃. After diffusion treatment at 850℃for 4 h, the distribution of aluminum and lanthanum elements in the coating was analyz