Injectable silk/hydroxyapatite nanocomposite hydrogels with vascularization capacity for bone regene

来源 :材料科学技术(英文版) | 被引量 : 0次 | 上传用户:userpanphilip
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
Localized and sustained osteogenic-angiogenic stimulation to bone defects is critical for effective bone repair.Here,desferrioxamine (DFO) was loaded on silk fibroin nanofibers and blended with hydroxyapatite nanorods (HA),forming injectable DFO-loaded silk fibroin-HA nanocomposite hydrogels.The composite hydrogels remained homogeneous distribution of HA with high ratio (60 %) and also higher stiffness than that of pure silk fibroin nanofiber hydrogels,which provided stable osteogenic stimulation niches for tissue regeneration.Without the scarify of injectability,the hydrogels achieved slow delivery of DFO for above 60 days,resulting in suitable angiogenesis in vitro and in vivo and better osteogenesis than DFO-free systems.Compared to previous injectable silk fibroin-HA hydrogels,the introduction of vascularization capacity further stimulated the osteogenic differentiation of stem cells and accelerated new bone formation.Quicker and better bone healing were detected at defect sites after the injection of DFO-loaded nanocomposite hydrogels,indicating the effective synergistic effect of osteogenic and angiogenic cues.This work provides a simple and effective strategy of introducing angiogenic cues to bone matrices.We believe that the injectable nanocomposite hydrogels are suitable for the regeneration of bone tissues.
其他文献
Although an increasing interest has been attracted to further develop heterostructured catalysts from metallic glasses(MGs)by heat treatment,overcoming surface
以聚乙烯吡咯烷酮(PVP)为模板采用静电纺丝法并结合高温煅烧制备出二维CdO纳米棒,用SEM、TGA、DSC、FT-IR及XRD等手段对产物的形貌和结构进行了表征.结果表明,所得纳米棒为纯
以3-氨基苯酚/甲醛(AF)树脂为软模板、正硅酸乙酯(TEOS)为硅源、十六烷基三甲基溴化铵(CTAB)为制孔剂,采用一锅溶胶-凝胶法制备中空介孔二氧化硅(HMS)微球.通过改变反应温度
用磁控溅射在硅片上制备MoS2和 Ti-MoS2薄膜,并将其在恒温恒湿箱中在AT 30℃、RH 70%条件下存储360 h.使用XRD谱、XPS谱和紫外-可见分光光度计、四探针测试仪表征分析薄膜的结
用CVD法制备的碳纳米管(CNTs)之间的相互吸引,将其堆叠成具有网状结构、多孔及高活性等优点的CNT海绵体(CNTS).于是,硫蒸气可在CNTs管束上形核沉积并与其紧密接触,使正极电子