论文部分内容阅读
摘要:随着现代化建设的不断发展,我国基础设施建设正以前所未有的规模在全国展开,同时质量问题越来越成为人们关注的焦点,近年来,频繁出现一些质量事故直接关系到人民群众生命财产安全,引起有关部门的高度重视。本文笔者通过对质量通病的研究分析,提出一些防治措施,以供参考。
关键词:公路工程;质量通病;预控
Abstract: With the development of modern construction, China''s infrastructure construction is on an unprecedented scale nationwide. However, at the same time, the quality problems draw more and more attention. In recent years, some quality accidents occured frequently directly relate to the safety of the lives and property of the public, causing much attention by the relevant departments. In this paper, based on the analysis of the common faults, the author puts forward some prevention and control measures for your reference.
Keywords: the highway engineering; the common faults; precontrol
中图分类号: F540.3 文献标识码:A文章编号:
对于公路建设,由于多年来工程质量通病具有极大的危害性和一定的顽固性,因此加强质量通病的研究和预控是一项重要的任务。
交通部风懋润总工程师曾专门撰文总结分析了高等级公路路基路面的六项质量通病及其原因:"(1)软弱地基路段预压时间不够,工后沉降过大,路面产生较大的不平整和横向裂缝;路基压实度不够和地基处理不当,引起路面产生较多纵向裂缝(沥青路面)或断板(刚性路面);构造物两端填土压实度不够,引起桥头跳车。(2)雨水进入面层引起面层网裂、变形和局部松散而形成坑洞;雨水透过面层滞留在基层顶面和基层质量不好引起冲刷唧浆、网裂、变形和坑洞,这种现象较多。(3)半刚性结构层厚度不足和工艺水平低,使路面产生早期结构性破坏;基层工艺水平不高,平整度差,使沥青面层厚薄相差较大,引起路面平整度较快降低。(4)面层采用质量不符合要求的沥青,以及基层材料设计和工艺不合适等原因,使面层横向裂缝过多。(5)面层粒料级配不佳和沥青用量不稳定,开放交通1~2年,行车道就产生轻重不一的泛油现象,使表面粗糙度显著下降,抗滑性能衰减较快,这种现象相当普遍。(6)沥青混合料矿料级配不佳,细料和沥青用量偏多,使路面产生严重辙槽(车辆大型化和严重超载也是原因之一)"。
下面对张家口地区常见的八项工程质量通病进行逐一分析,供有关方面参考。
一、防护工程和结构物表面粗糙
混凝土结构物表面不光滑,外观不美观,这在张家口地区尤其严重,与其它先进省市相比差距很大。应采用以下方法进行预防:
(1)模板面要清理干净。(2)尽量采用刚度好的大模板,浇注混凝土前应用清水将模板湿洗干净,不留积水,模板缝应拼严,控制跑模,防止漏浆。(3)钢模隔离剂涂刷均匀,不得漏刷。(4)加强混凝土配合比设计和生产过程中的质量管理,重视外掺剂的使用研究。(5)混凝土振捣要密实,应不漏振不过振。
二、高填土下沉
深填、高填、半填半挖、桥头引道高填土或立交桥互通匝道填方,往往会在通车一段时间后下沉,究其原因,一方面在于施工因素,如压实控制不好、分层过厚、冬施措施不当等,另一方面在于材料因素,如最大干容重及最佳含水量有误、材料压缩系数过大、采用高塑性指数的粘性土等,均会出现此问题,它会使路面变形、开裂或下陷。在工程中宜采用以下措施予以控制:
(1)按路面平行线分层控制填土标高,按试验路路基填土厚度的90%来控制规模施工时的填土厚度。(2)在新旧填土的衔接处,严格控制填土接茬台阶的最小长度,以避免接茬处超厚,压实不足。(3)防止漏夯或夯实不足,严禁超厚填土。(4)在机械难于压实的地方,用适当的小型机具进行补充夯实。(5)冬季施工时应使土在未受冻的情况下回填压实,避免填土压实密度严重不均匀而造成土体下沉。(6)回填几种土时,不能仅用某一种土的击实试验得出的密度标准作为所有填土的压实度标准,而应按填土的不同类别,做相应土的若干组击实试验,取值应符合相应规定。
三、沥青路面早期破损
是指路面在竣工后通车不久或一、两年内出现多处或大面积裂缝、破损。其原因主要有:施工控制问题。目前,路面工程片面追求平整度,而忽视压实度的要求;材料到场及终压温度偏低,甚至在低温情况下过度碾压;材料配合比不当,基质沥青未达标;路面基层甚至路床、基底承载力不足,弯沉值过大。碾压中产生的细微裂纹及反射裂缝虽初期不影响行车,但在水分侵蚀及阳光照射下,成为促使面层沥青混凝土疲劳开裂的催化剂,大大缩短沥青路面寿命。
四、桥梁伸缩缝和桥头跳车
由于桥头填土的沉降与桥台沉降有差异,以及伸缩缝、桥头搭板做得不好,在桥台处形成台阶,影响行车的舒适和安全,并对桥梁产生很大的冲击力。在施工过程中应注意以下几点:
(1)桥台后背填土应选用排水和压实性能好的回填材料,以达到最好的压实度,减少路堤填土的沉降量。(2)对于桩柱式桥台,应先填方,待填方充分沉降后,再修建桩柱式桥台,从而减少结构物与填土的沉降差。(3)选用性能好的伸缩缝,并精心施工,以保证桥面伸缩缝处的平整完好。(4)采用有效措施尽量减少桥面铺装层的裂缝。(5)做好桥头搭板或采用土工格栅等新技术进行过渡。
五、软土地基超限沉陷
软土具有含水量大、抗剪强度低、承载能力低的特性。在软土上修建路基或桥涵构造物基础易出现压缩沉降、滑陷、坍塌等,对软土地基主要采取以下方法:
(1)采用换填渗水性良好的土,对基底进行加固。(2)设置白灰粗砂桩,此法适用于粉砂土质、含水量大的软土地基。软土地基成孔后,筛选生石灰块加水泥、粗砂拌匀后填充,用木棍捣实,当生石灰块遇地下水消解后,填充料体积膨胀,起到挤压土基作用,提高了路基承载力。(3)石灰、水泥稳定碎石法:是用于苇塘、稻田、藕池的沼泽地区路基的处理。排水、清淤、清除草根植被后,将石灰和水泥混合,再将碎石与混合料拌和均匀,然后摊铺压实养护。(4)对路基采取强夯、预压等措施或使用土工织物。
六、预应力结构孔道压浆不实
由于灌浆强度低,在孔道内填充不饱满,易产生预应力钢筋的锈蚀,对于通过灌浆握裹钢材来传递预加应力给结构混凝土的作用将有所削弱。故施工时应采取以下方法进行控制:
(1)灌浆用的水泥应是新出厂的,标号不低于425#的硅酸盐水泥或普通硅酸盐水泥。(2)灰浆的配合比,必须结合施工季节、使用材料、现场条件等灵活选取,并通过试配试验确定。(3)灌注前应检查灌注通道的管道状态是否通畅,对孔道应在灌注前用压力水冲洗。(4)张拉后应尽早进行孔道压浆,压浆应缓慢、均匀、连续进行。(5)每孔道应一次灌成,中途不应停顿。
七、路面不平
路面平整度是公路工程的主要舒适性指标,施工控制不好,平整度衰减很快。如果道路不平,会降低车速,增加行车颠簸,加大冲击力,损坏车辆,降低舒适性,减少安全性,降低经济效益和社会效益。出现的主要原因有:基層平整度控制不严,甚至出现波浪式起伏;路面施工控制不力,摊铺机及压路机的操作人员水平较低;基准线或滑靴失控,从目前路面施工情况看,滑靴已基本取代基准线但仍有其局限性。
总之,公路工程质量通病的治理必须思想上重视、管理上及时、技术上合理、措施上得力,建设、设计、监理、施工各方面、各环节齐抓共管,才能使我们的质量有根本的改观,才能建成精品工程。
关键词:公路工程;质量通病;预控
Abstract: With the development of modern construction, China''s infrastructure construction is on an unprecedented scale nationwide. However, at the same time, the quality problems draw more and more attention. In recent years, some quality accidents occured frequently directly relate to the safety of the lives and property of the public, causing much attention by the relevant departments. In this paper, based on the analysis of the common faults, the author puts forward some prevention and control measures for your reference.
Keywords: the highway engineering; the common faults; precontrol
中图分类号: F540.3 文献标识码:A文章编号:
对于公路建设,由于多年来工程质量通病具有极大的危害性和一定的顽固性,因此加强质量通病的研究和预控是一项重要的任务。
交通部风懋润总工程师曾专门撰文总结分析了高等级公路路基路面的六项质量通病及其原因:"(1)软弱地基路段预压时间不够,工后沉降过大,路面产生较大的不平整和横向裂缝;路基压实度不够和地基处理不当,引起路面产生较多纵向裂缝(沥青路面)或断板(刚性路面);构造物两端填土压实度不够,引起桥头跳车。(2)雨水进入面层引起面层网裂、变形和局部松散而形成坑洞;雨水透过面层滞留在基层顶面和基层质量不好引起冲刷唧浆、网裂、变形和坑洞,这种现象较多。(3)半刚性结构层厚度不足和工艺水平低,使路面产生早期结构性破坏;基层工艺水平不高,平整度差,使沥青面层厚薄相差较大,引起路面平整度较快降低。(4)面层采用质量不符合要求的沥青,以及基层材料设计和工艺不合适等原因,使面层横向裂缝过多。(5)面层粒料级配不佳和沥青用量不稳定,开放交通1~2年,行车道就产生轻重不一的泛油现象,使表面粗糙度显著下降,抗滑性能衰减较快,这种现象相当普遍。(6)沥青混合料矿料级配不佳,细料和沥青用量偏多,使路面产生严重辙槽(车辆大型化和严重超载也是原因之一)"。
下面对张家口地区常见的八项工程质量通病进行逐一分析,供有关方面参考。
一、防护工程和结构物表面粗糙
混凝土结构物表面不光滑,外观不美观,这在张家口地区尤其严重,与其它先进省市相比差距很大。应采用以下方法进行预防:
(1)模板面要清理干净。(2)尽量采用刚度好的大模板,浇注混凝土前应用清水将模板湿洗干净,不留积水,模板缝应拼严,控制跑模,防止漏浆。(3)钢模隔离剂涂刷均匀,不得漏刷。(4)加强混凝土配合比设计和生产过程中的质量管理,重视外掺剂的使用研究。(5)混凝土振捣要密实,应不漏振不过振。
二、高填土下沉
深填、高填、半填半挖、桥头引道高填土或立交桥互通匝道填方,往往会在通车一段时间后下沉,究其原因,一方面在于施工因素,如压实控制不好、分层过厚、冬施措施不当等,另一方面在于材料因素,如最大干容重及最佳含水量有误、材料压缩系数过大、采用高塑性指数的粘性土等,均会出现此问题,它会使路面变形、开裂或下陷。在工程中宜采用以下措施予以控制:
(1)按路面平行线分层控制填土标高,按试验路路基填土厚度的90%来控制规模施工时的填土厚度。(2)在新旧填土的衔接处,严格控制填土接茬台阶的最小长度,以避免接茬处超厚,压实不足。(3)防止漏夯或夯实不足,严禁超厚填土。(4)在机械难于压实的地方,用适当的小型机具进行补充夯实。(5)冬季施工时应使土在未受冻的情况下回填压实,避免填土压实密度严重不均匀而造成土体下沉。(6)回填几种土时,不能仅用某一种土的击实试验得出的密度标准作为所有填土的压实度标准,而应按填土的不同类别,做相应土的若干组击实试验,取值应符合相应规定。
三、沥青路面早期破损
是指路面在竣工后通车不久或一、两年内出现多处或大面积裂缝、破损。其原因主要有:施工控制问题。目前,路面工程片面追求平整度,而忽视压实度的要求;材料到场及终压温度偏低,甚至在低温情况下过度碾压;材料配合比不当,基质沥青未达标;路面基层甚至路床、基底承载力不足,弯沉值过大。碾压中产生的细微裂纹及反射裂缝虽初期不影响行车,但在水分侵蚀及阳光照射下,成为促使面层沥青混凝土疲劳开裂的催化剂,大大缩短沥青路面寿命。
四、桥梁伸缩缝和桥头跳车
由于桥头填土的沉降与桥台沉降有差异,以及伸缩缝、桥头搭板做得不好,在桥台处形成台阶,影响行车的舒适和安全,并对桥梁产生很大的冲击力。在施工过程中应注意以下几点:
(1)桥台后背填土应选用排水和压实性能好的回填材料,以达到最好的压实度,减少路堤填土的沉降量。(2)对于桩柱式桥台,应先填方,待填方充分沉降后,再修建桩柱式桥台,从而减少结构物与填土的沉降差。(3)选用性能好的伸缩缝,并精心施工,以保证桥面伸缩缝处的平整完好。(4)采用有效措施尽量减少桥面铺装层的裂缝。(5)做好桥头搭板或采用土工格栅等新技术进行过渡。
五、软土地基超限沉陷
软土具有含水量大、抗剪强度低、承载能力低的特性。在软土上修建路基或桥涵构造物基础易出现压缩沉降、滑陷、坍塌等,对软土地基主要采取以下方法:
(1)采用换填渗水性良好的土,对基底进行加固。(2)设置白灰粗砂桩,此法适用于粉砂土质、含水量大的软土地基。软土地基成孔后,筛选生石灰块加水泥、粗砂拌匀后填充,用木棍捣实,当生石灰块遇地下水消解后,填充料体积膨胀,起到挤压土基作用,提高了路基承载力。(3)石灰、水泥稳定碎石法:是用于苇塘、稻田、藕池的沼泽地区路基的处理。排水、清淤、清除草根植被后,将石灰和水泥混合,再将碎石与混合料拌和均匀,然后摊铺压实养护。(4)对路基采取强夯、预压等措施或使用土工织物。
六、预应力结构孔道压浆不实
由于灌浆强度低,在孔道内填充不饱满,易产生预应力钢筋的锈蚀,对于通过灌浆握裹钢材来传递预加应力给结构混凝土的作用将有所削弱。故施工时应采取以下方法进行控制:
(1)灌浆用的水泥应是新出厂的,标号不低于425#的硅酸盐水泥或普通硅酸盐水泥。(2)灰浆的配合比,必须结合施工季节、使用材料、现场条件等灵活选取,并通过试配试验确定。(3)灌注前应检查灌注通道的管道状态是否通畅,对孔道应在灌注前用压力水冲洗。(4)张拉后应尽早进行孔道压浆,压浆应缓慢、均匀、连续进行。(5)每孔道应一次灌成,中途不应停顿。
七、路面不平
路面平整度是公路工程的主要舒适性指标,施工控制不好,平整度衰减很快。如果道路不平,会降低车速,增加行车颠簸,加大冲击力,损坏车辆,降低舒适性,减少安全性,降低经济效益和社会效益。出现的主要原因有:基層平整度控制不严,甚至出现波浪式起伏;路面施工控制不力,摊铺机及压路机的操作人员水平较低;基准线或滑靴失控,从目前路面施工情况看,滑靴已基本取代基准线但仍有其局限性。
总之,公路工程质量通病的治理必须思想上重视、管理上及时、技术上合理、措施上得力,建设、设计、监理、施工各方面、各环节齐抓共管,才能使我们的质量有根本的改观,才能建成精品工程。