The performance of severe oxidation of methanol on 0.1%Pd supported on alumina was studied by a combined device of chromatograph-micro reactor. The results show that the addition of La into γ-Al 2O 3 as support can affect the performance of Pd catalyst greatly. By using Pd catalyst containing La in methanol oxidation, though, the ignition temperature is not lower than that by using Pd catalyst, the presence of La does suppress the formation of oxygenic intermediates. The results by in-situ FTIR show that the presence of La in the support affects the adsorbed species and hence the mechanism of severe oxidation of methanol on Pd catalyst.
The performance of severe oxidation of methanol on 0.1% Pd supported on alumina was studied by a combined device of chromatograph-micro reactor. The results show that the addition of La to γ-Al 2 O 3 as support can affect the performance of Pd catalyst greatly . By using Pd catalyst containing La in methanol oxidation, though, the ignition temperature is not lower than that by using Pd catalyst, the presence of La does suppress the formation of oxygenic intermediates. The results by in-situ FTIR show that the presence of La in the support affects the adsorbed species and hence the mechanism of severe oxidation of methanol on Pd catalyst.