日本《钢铁界报》七月一日刊载题为《世界最高水准的高炉燃料比》的文章,摘要如下: 高炉燃料比是表明高炉经济性的重要指标。在过去二十年中,日本燃料比从九百一十五公斤降至四百九十五公斤。降低燃料比的技术有: 一、高炉入炉料的改善 炉料的尺寸应能使炉内反应快而且透气性良好。目前块矿经破碎、筛分后,粒度下限为八至十毫米,上限为二十五至三十毫米。对烧结矿和焦炭也筛除粉末,并规定粒度上限。 Japan’s “Iron and Steel Tribune,” July 1 published an article entitled “the world’s highest level of blast furnace fuel ratio,” the article is summarized as follows: Blast furnace fuel ratio is an important indicator of blast furnace economy. In the past two decades, Japan’s fuel ratio has dropped from 915 kilograms to 495 kilograms. Techniques to reduce the fuel ratio are: First, the blast furnace into the charge to improve the size of the charge should be able to make the furnace reaction fast and good air permeability. At present, lump ore is crushed and sieved, the grain size lower limit is eight to ten millimeters and the upper limit is twenty-five to thirty millimeters. Sinter and coke also screen the powder, and provides the upper limit of particle size.
其他文献
我厂在浮选辉钼矿过程中,使用水玻璃作为硅酸盐和碳酸盐矿泥的分散剂和抑制剂,添加在搅拌槽和浮选机中,已经多年。1967年为解决松北矿石磨矿分级溢流的“高浓度、低细度”的
用高温离心法确定了电炉渣中镍的损失形式:当渣含镍>0.15%时,以夹杂损失为主,所占比例为51~79%;渣含镍
安阳钢铁厂水冶炼铁分厂是拥有四座100米~3高炉的单一炼铁厂。高炉使用的含铁原料以“平地吹”土烧结矿为主,还有一座8米~2竖炉生产的高氧化镁自熔性球团矿。高炉使用的焦炭
2005年3月,福州市晋安区工商局以福州南方建材市场中的陶瓷洁具市场为试点,实行了市场业主责任制,明确市场业主(即开办者)是市场管理的第一责任人,指导市场业主建立了一系列
俄罗斯国防部长谢尔久科夫与“米格”飞机制造公司总经理签订合同,采购24家米格-29K/КУБ型舰载机。根据协议,俄罗斯国防部将在2012~2015年间接收20架米格-29K和4架米格-29
作者经过大冶有色金属公司冶炼厂技术改造的可行性研究。认为用氧气喷吹熔炼是改造大冶反射炉较好的方案,它具有以下优点:技术进步、基本上利用原有设备,国外已有工业生产的
1983年全国转炉炼钢会议上,已将LD转炉静态、动态控制列为重点科研项目。因此,本文特对LD转炉静态、动态过程控制的发展趋势作一分析;并对副枪动态控制、副枪加炉气动态控制
75硅铁冒瘤会对产品质量产生严重影响,目前各厂家都在采取切实可行的工艺措施来防止。现仅就我厂的工作情况叙述如下: 一、原因分析所谓冒瘤,即在75硅铁铸锭过程中,铁锭 Fe
在大多数钢中,磷是有害杂质,但在某些情况下,磷又有特殊的作用。如轧辊钢加入0.4—0.5%的磷,可改善其流动性和避免表面裂纹。客货车闸瓦含磷0.7—1.0%,能提高其耐磨性能。磷还
我厂的电钴生产中,采用N235萃取分离钴镍。由于有机相夹带,洗镍不彻底,因而钴镍比只能达到生产2号钴的要求;有时还往往达不到。这部分钴液由于Cl~-低,Co高,不利于再进行镍钴