Wood of Chinese fir and poplar were liquefied in phenol at 150℃ and atmospheric pressure. The liquefied wood were react......
采用苯酚和聚乙二醇400复合液化试剂,对竹材加工剩余物进行液化和液化产物的树脂化试验。采用单因素法,探讨主要工艺因素对液化效果......