The quantitative adsorption behavior of a hyperdispersant onto nano-TiO2 particles has been characterized by using FTIR (Fourier transform infrared) spectroscop
Glass formation is generally favored by a large atomic size mismatch among constituent elements, which usually leads to large density differences among them as
A series of 60 nm thick indium oxide thin-films, all amorphous as determined by x-ray diffraction, were found to have physical and electrical properties that de